2022Additive Manufacturing LettersOpen access

Mitigating keyhole pore formation by nanoparticles during laser powder bed fusion additive manufacturing

Minglei Qu, Qilin Guo, Luis I. Escano, Samuel J. Clark, Kamel Fezzaa, Lianyi Chen

Open full text 57 citations

Abstract

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.

Open-access reader

About this research paper

What this paper is about

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.

Why it matters

OpenAlex reports 57 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.

Key concepts: Keyhole, Materials science, Nanoparticle, Chemical engineering, Nanotechnology, Composite material, Welding, Engineering

Related papers

Back to paper searchBrowse research topicsOriginal source
Mitigating keyhole pore formation by nanoparticles during laser powder bed fusion additive manufacturing — Research Paper | ScholarLens