2014•China ElastomericsRequires access

Effect of vulcanization system on properties of pilot product EPDM of Yan Hua

Xie Xiaoran, Hongliang Qu, Ruixian Zhang

Open publisher page 0 citations

Abstract

研究了硫黄硫化体系和过氧化物体系对燕化中试产品三元乙丙橡胶(EPDM)性能的影响.实验结果表明,硫黄硫化体系中硫黄用量为1.5份时胶料物理机械性能最好;硫黄用量为2份时,胶料耐热老化性能最好.硫黄硫化体系中,二硫化四基秋兰姆(TMTDM)、2硫醇基苯并噻唑(M)和N-环己基-2-苯并噻唑次磺酸胺(CZ)3种促进剂并用时协同作用较好,胶料硫化速度最快,力学性能最好;促进剂TMTD用量为1.5份时,胶料压缩永久变形最小,耐热性能最好.过氧化物硫化体系中,当DCP用量由2份增加至5份时,胶料硫化速度提高,力学性能下降,压缩永久变形性能有一定改善.三烯丙基异氰脲酸酯(TALC)用量为5份时,胶料压缩永久变形最小,耐热氧老化性能最好.

About this research paper

What this paper is about

研究了硫黄硫化体系和过氧化物体系对燕化中试产品三元乙丙橡胶(EPDM)性能的影响.实验结果表明,硫黄硫化体系中硫黄用量为1.5份时胶料物理机械性能最好;硫黄用量为2份时,胶料耐热老化性能最好.硫黄硫化体系中,二硫化四基秋兰姆(TMTDM)、2硫醇基苯并噻唑(M)和N-环己基-2-苯并噻唑次磺酸胺(CZ)3种促进剂并用时协同作用较好,胶料硫化速度最快,力学性能最好;促进剂TMTD用量为1.5份时,胶料压缩永久变形最小,耐热性能最好.过氧化物硫化体系中,当DCP用量由2份增加至5份时,胶料硫化速度提高,力学性能下降,压缩永久变形性能有一定改善.三烯丙基异氰脲酸酯(TALC)用量为5份时,胶料压缩永久变形最小,耐热氧老化性能最好.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

研究了硫黄硫化体系和过氧化物体系对燕化中试产品三元乙丙橡胶(EPDM)性能的影响.实验结果表明,硫黄硫化体系中硫黄用量为1.5份时胶料物理机械性能最好;硫黄用量为2份时,胶料耐热老化性能最好.硫黄硫化体系中,二硫化四基秋兰姆(TMTDM)、2硫醇基苯并噻唑(M)和N-环己基-2-苯并噻唑次磺酸胺(CZ)3种促进剂并用时协同作用较好,胶料硫化速度最快,力学性能最好;促进剂TMTD用量为1.5份时,胶料压缩永久变形最小,耐热性能最好.过氧化物硫化体系中,当DCP用量由2份增加至5份时,胶料硫化速度提高,力学性能下降,压缩永久变形性能有一定改善.三烯丙基异氰脲酸酯(TALC)用量为5份时,胶料压缩永久变形最小,耐热氧老化性能最好.

Key concepts: Vulcanization, Materials science, Composite material, EPDM rubber, Polymer science, Natural rubber

Related papers

Back to paper searchBrowse research topicsOriginal source
Effect of vulcanization system on properties of pilot product EPDM of Yan Hua — Research Paper | ScholarLens