2020•MineralsOpen access

Thermal Beneficiation of Sra Ouertane (Tunisia) Low-Grade Phosphate Rock

Noureddine Abbès, Essaïd Bilal, Ludwig Hermann, Gerald Steiner, Nils Hendrik Haneklaus

Open full text 25 citations

Abstract

Low-grade phosphate rock from Sra Ouertane (Tunisia) was beneficiated using a thermal treatment consisting of calcination, quenching, and disliming. Untreated phosphate rock samples (group 1), calcined phosphate rock samples (group 2), as well as calcined, quenched, and dislimed (group 3) phosphate rock samples, were investigated using inductively-coupled plasma atomic emission spectroscopy (ICP-AES), inductively-coupled plasma mass spectrometry (ICP-MS), thermogravimetric analysis (TGA), and X-ray powder diffraction (XRD). Besides, the particle size distribution of the aforementioned three groups was determined. The proposed thermal treatment successfully increased the P2O5 content of the untreated phosphate rock from 20.01 wt% (group 1) to 24.24 wt% (group 2) after calcination and, finally, 27.24 wt% (group 3) after calcination, quenching, and disliming. It was further found that the concentration of relevant accompanying rare earth elements (Ce, La, Nd, Pr, Sm, and Y) was increased and that the concentration of Cd could be significantly reduced from 30 mg/kg to 14 mg/kg with the proposed treatment. The resulting phosphate concentrate showed relatively high concentrations in metal oxides: Ʃ MgO, Fe2O3, Al2O3 = 3.63 wt% and silica (9.81 wt%) so that it did not meet the merchant grade specifications of a minimum P2O5 content of 30 wt% yet. Removal of these elements could be achieved using additional appropriate separation techniques.

Open-access reader

About this research paper

What this paper is about

Low-grade phosphate rock from Sra Ouertane (Tunisia) was beneficiated using a thermal treatment consisting of calcination, quenching, and disliming. Untreated phosphate rock samples (group 1), calcined phosphate rock samples (group 2), as well as calcined, quenched, and dislimed (group 3) phosphate rock samples, were investigated using inductively-coupled plasma atomic emission spectroscopy (ICP-AES), inductively-coupled plasma mass spectrometry (ICP-MS), thermogravimetric analysis (TGA), and X-ray powder diffraction (XRD). Besides, the particle size distribution of the aforementioned three groups was determined. The proposed thermal treatment successfully increased the P2O5 content of the untreated phosphate rock from 20.01 wt% (group 1) to 24.24 wt% (group 2) after calcination and, finally, 27.24 wt% (group 3) after calcination, quenching, and disliming. It was further found that the concentration of relevant accompanying rare earth elements (Ce, La, Nd, Pr, Sm, and Y) was increased and that the concentration of Cd could be significantly reduced from 30 mg/kg to 14 mg/kg with the proposed treatment. The resulting phosphate concentrate showed relatively high concentrations in metal oxides: Ʃ MgO, Fe2O3, Al2O3 = 3.63 wt% and silica (9.81 wt%) so that it did not meet the merchant grade specifications of a minimum P2O5 content of 30 wt% yet. Removal of these elements could be achieved using additional appropriate separation techniques.

Why it matters

OpenAlex reports 25 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Low-grade phosphate rock from Sra Ouertane (Tunisia) was beneficiated using a thermal treatment consisting of calcination, quenching, and disliming. Untreated phosphate rock samples (group 1), calcined phosphate rock samples (group 2), as well as calcined, quenched, and dislimed (group 3) phosphate rock samples, were investigated using inductively-coupled plasma atomic emission spectroscopy (ICP-AES), inductively-coupled plasma mass spectrometry (ICP-MS), thermogravimetric analysis (TGA), and X-ray powder diffraction (XRD). Besides, the particle size distribution of the aforementioned three groups was determined. The proposed thermal treatment successfully increased the P2O5 content of the untreated phosphate rock from 20.01 wt% (group 1) to 24.24 wt% (group 2) after calcination and, finally, 27.24 wt% (group 3) after calcination, quenching, and disliming. It was further found that the concentration of relevant accompanying rare earth elements (Ce, La, Nd, Pr, Sm, and Y) was increased and that the concentration of Cd could be significantly reduced from 30 mg/kg to 14 mg/kg with the proposed treatment. The resulting phosphate concentrate showed relatively high concentrations in metal oxides: Ʃ MgO, Fe2O3, Al2O3 = 3.63 wt% and silica (9.81 wt%) so that it did not meet the merchant grade specifications of a minimum P2O5 content of 30 wt% yet. Removal of these elements could be achieved using additional appropriate separation techniques.

Key concepts: Calcination, Beneficiation, Thermogravimetric analysis, Phosphate, Inductively coupled plasma mass spectrometry, Inductively coupled plasma, Nuclear chemistry, Inductively coupled plasma atomic emission spectroscopy

Related papers

Back to paper searchBrowse research topicsOriginal source
Thermal Beneficiation of Sra Ouertane (Tunisia) Low-Grade Phosphate Rock — Research Paper | ScholarLens