Deformation twinning behavior in Fe-17Mn-0.6C, Fe-17Mn-0.8C, and Fe-18Mn-1.2C (wt.%) twinning-induced plasticity (TWIP) steels was investigated by atomic force microscopy (AFM) and electron backscatter diffraction pattern (EBSD) analyses. The AFM-based surface relief analysis combined with the EBSD measurements was employed to determine active twinning direction as well as deformation twin fraction in specific crystallographic orientations. A carbon addition is known to increase the stacking fault energy; however the deformation twin fraction in the <144> tensile orientation did not change against carbon concentration. On one hand, the <111> tensile orientation grains showed suppression of deformation twinning with increasing carbon concentration. These results imply that another factor in addition to the stacking fault energy-based criteria is required to interpret the deformation twinning behavior of carbon-added TWIP steels.

Open-access reader

About this research paper

What this paper is about

Deformation twinning behavior in Fe-17Mn-0.6C, Fe-17Mn-0.8C, and Fe-18Mn-1.2C (wt.%) twinning-induced plasticity (TWIP) steels was investigated by atomic force microscopy (AFM) and electron backscatter diffraction pattern (EBSD) analyses. The AFM-based surface relief analysis combined with the EBSD measurements was employed to determine active twinning direction as well as deformation twin fraction in specific crystallographic orientations. A carbon addition is known to increase the stacking fault energy; however the deformation twin fraction in the <144> tensile orientation did not change against carbon concentration. On one hand, the <111> tensile orientation grains showed suppression of deformation twinning with increasing carbon concentration. These results imply that another factor in addition to the stacking fault energy-based criteria is required to interpret the deformation twinning behavior of carbon-added TWIP steels.

Why it matters

OpenAlex reports 8 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Deformation twinning behavior in Fe-17Mn-0.6C, Fe-17Mn-0.8C, and Fe-18Mn-1.2C (wt.%) twinning-induced plasticity (TWIP) steels was investigated by atomic force microscopy (AFM) and electron backscatter diffraction pattern (EBSD) analyses. The AFM-based surface relief analysis combined with the EBSD measurements was employed to determine active twinning direction as well as deformation twin fraction in specific crystallographic orientations. A carbon addition is known to increase the stacking fault energy; however the deformation twin fraction in the <144> tensile orientation did not change against carbon concentration. On one hand, the <111> tensile orientation grains showed suppression of deformation twinning with increasing carbon concentration. These results imply that another factor in addition to the stacking fault energy-based criteria is required to interpret the deformation twinning behavior of carbon-added TWIP steels.

Key concepts: Twip, Crystal twinning, Electron backscatter diffraction, Materials science, Stacking-fault energy, Deformation (meteorology), Plasticity, Deformation mechanism

Related papers

Back to paper searchBrowse research topicsOriginal source
Deformation Twinning Behavior of Twinning-Induced Plasticity Steels with Different Carbon Concentrations — Research Paper | ScholarLens