2020Structural ConcreteRequires access

Experimental study on mechanical behavior of thermally damaged grouted sleeve splice under cyclic loading

Jianzhuang Xiao, Lianglin Liu, Tao Ding, Qinghai Xie

Open publisher page 30 citations

Abstract

Abstract An experimental program concerning 48 specimens of grouted sleeve splices, first heated up to 600°C and then subjected to cyclic loading was presented and discussed in this study. Similar rebar splices were often used in the precast concrete structures designed for seismic regions. The temperature of the splice and the compressive strength of the grout were the main variables considered in this study. It is found that the temperature mainly affected the peak bearing capacity of the grout and the failure pattern of the connection. In fact, the typical failure pattern at room temperature (rebar fracture outside the sleeve) turned to rebar pullout of the sleeve above 400°C, which indicated that below this temperature grout‐to‐rebar bond kept most of its original efficacy. On the contrary, bond failure occurred for all specimens at 600°C because of rebar slip. A calculation method was proposed as well to evaluate the peak bearing capacity of grouted sleeve splice, based on the load transferring mechanisms of the bond between grout‐to‐rebar and sleeve‐to‐grout. The conducted experimental study and analysis provide a better understanding on the bond mechanism of thermally damaged grouted sleeve splices subjected to cyclic loading.

About this research paper

What this paper is about

Abstract An experimental program concerning 48 specimens of grouted sleeve splices, first heated up to 600°C and then subjected to cyclic loading was presented and discussed in this study. Similar rebar splices were often used in the precast concrete structures designed for seismic regions. The temperature of the splice and the compressive strength of the grout were the main variables considered in this study. It is found that the temperature mainly affected the peak bearing capacity of the grout and the failure pattern of the connection. In fact, the typical failure pattern at room temperature (rebar fracture outside the sleeve) turned to rebar pullout of the sleeve above 400°C, which indicated that below this temperature grout‐to‐rebar bond kept most of its original efficacy. On the contrary, bond failure occurred for all specimens at 600°C because of rebar slip. A calculation method was proposed as well to evaluate the peak bearing capacity of grouted sleeve splice, based on the load transferring mechanisms of the bond between grout‐to‐rebar and sleeve‐to‐grout. The conducted experimental study and analysis provide a better understanding on the bond mechanism of thermally damaged grouted sleeve splices subjected to cyclic loading.

Why it matters

OpenAlex reports 30 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Abstract An experimental program concerning 48 specimens of grouted sleeve splices, first heated up to 600°C and then subjected to cyclic loading was presented and discussed in this study. Similar rebar splices were often used in the precast concrete structures designed for seismic regions. The temperature of the splice and the compressive strength of the grout were the main variables considered in this study. It is found that the temperature mainly affected the peak bearing capacity of the grout and the failure pattern of the connection. In fact, the typical failure pattern at room temperature (rebar fracture outside the sleeve) turned to rebar pullout of the sleeve above 400°C, which indicated that below this temperature grout‐to‐rebar bond kept most of its original efficacy. On the contrary, bond failure occurred for all specimens at 600°C because of rebar slip. A calculation method was proposed as well to evaluate the peak bearing capacity of grouted sleeve splice, based on the load transferring mechanisms of the bond between grout‐to‐rebar and sleeve‐to‐grout. The conducted experimental study and analysis provide a better understanding on the bond mechanism of thermally damaged grouted sleeve splices subjected to cyclic loading.

Key concepts: Rebar, Grout, Precast concrete, Materials science, Structural engineering, Bearing capacity, Composite material, splice

Related papers

Back to paper searchBrowse research topicsOriginal source
Experimental study on mechanical behavior of thermally damaged grouted sleeve splice under cyclic loading — Research Paper | ScholarLens