2020MaterialsOpen access

Hot Deformation Behavior and Microstructure Evolution of Cu–Ni–Co–Si Alloys

Feng Liu, Jimiao Ma, Lijun Peng, Guojie Huang, Wenjing Zhang, Haofeng Xie, Xujun Mi

Open full text 17 citations

Abstract

The Cu-1.7Ni-1.4Co-0.65Si (wt%) alloy is hot compressed by a Gleeble-1500D machine under a temperature range of 760 to 970 °C and a strain rate range of 0.01 to 10 s−1. The flow stress increases with the extension of strain rate and decreases with the rising of deformation temperature. The dynamic recrystallization behavior happens during the hot compression deformation process. The hot deformation activation energy of the alloy can be calculated as 468.5 kJ/mol, and the high temperature deformation constitutive equation is confirmed. The hot processing map of the alloy is established on the basis of hot deformation behavior and hot working characteristics. With the optimal thermal deformation conditions of 940 to 970 °C and 0.01 to 10 s−1, the fine equiaxed grain and no holes are found in the matrix, which can provide significant guidance for hot deformation processing technology of Cu–Ni–Co–Si alloy.

Open-access reader

About this research paper

What this paper is about

The Cu-1.7Ni-1.4Co-0.65Si (wt%) alloy is hot compressed by a Gleeble-1500D machine under a temperature range of 760 to 970 °C and a strain rate range of 0.01 to 10 s−1. The flow stress increases with the extension of strain rate and decreases with the rising of deformation temperature. The dynamic recrystallization behavior happens during the hot compression deformation process. The hot deformation activation energy of the alloy can be calculated as 468.5 kJ/mol, and the high temperature deformation constitutive equation is confirmed. The hot processing map of the alloy is established on the basis of hot deformation behavior and hot working characteristics. With the optimal thermal deformation conditions of 940 to 970 °C and 0.01 to 10 s−1, the fine equiaxed grain and no holes are found in the matrix, which can provide significant guidance for hot deformation processing technology of Cu–Ni–Co–Si alloy.

Why it matters

OpenAlex reports 17 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The Cu-1.7Ni-1.4Co-0.65Si (wt%) alloy is hot compressed by a Gleeble-1500D machine under a temperature range of 760 to 970 °C and a strain rate range of 0.01 to 10 s−1. The flow stress increases with the extension of strain rate and decreases with the rising of deformation temperature. The dynamic recrystallization behavior happens during the hot compression deformation process. The hot deformation activation energy of the alloy can be calculated as 468.5 kJ/mol, and the high temperature deformation constitutive equation is confirmed. The hot processing map of the alloy is established on the basis of hot deformation behavior and hot working characteristics. With the optimal thermal deformation conditions of 940 to 970 °C and 0.01 to 10 s−1, the fine equiaxed grain and no holes are found in the matrix, which can provide significant guidance for hot deformation processing technology of Cu–Ni–Co–Si alloy.

Key concepts: Materials science, Dynamic recrystallization, Equiaxed crystals, Strain rate, Deformation (meteorology), Flow stress, Hot working, Alloy

Related papers

Back to paper searchBrowse research topicsOriginal source
Hot Deformation Behavior and Microstructure Evolution of Cu–Ni–Co–Si Alloys — Research Paper | ScholarLens