Abstract

Zeolite-filled polydimethylsiloxane (PDMS) mixed matrix membranes (MMMs) were developed for pervaporation separation of n -butanol from dilute butanol–water solution. The effects of zeolite, feed butanol concentration, and temperature were studied. In general, the butanol separation factor increased with increasing the temperature, whereas the fluxes increased with the reducing membrane thickness and increasing feed butanol concentration and temperature. At 47 °C, PDMS MMMs filled with 40 wt % zeolite gave the highest separation factor of 77, which would reduce the energy consumption for butanol recovery from 1.0 wt % butanol by ∼75% to ∼10 MJ/kg butanol using a hybrid pervaporation-distillation process compared to distillation. The zeolite-filled PDMS MMM with a thickness of 10 μm would have a high butanol flux of 1000 g/m 2 ·h at 56 °C. With a high separation factor and butanol flux, the zeolite-filled PDMS MMM would be advantageous for recovering n -butanol from dilute solution at significantly reduced energy input and cost.

About this research paper

What this paper is about

Zeolite-filled polydimethylsiloxane (PDMS) mixed matrix membranes (MMMs) were developed for pervaporation separation of n -butanol from dilute butanol–water solution. The effects of zeolite, feed butanol concentration, and temperature were studied. In general, the butanol separation factor increased with increasing the temperature, whereas the fluxes increased with the reducing membrane thickness and increasing feed butanol concentration and temperature. At 47 °C, PDMS MMMs filled with 40 wt % zeolite gave the highest separation factor of 77, which would reduce the energy consumption for butanol recovery from 1.0 wt % butanol by ∼75% to ∼10 MJ/kg butanol using a hybrid pervaporation-distillation process compared to distillation. The zeolite-filled PDMS MMM with a thickness of 10 μm would have a high butanol flux of 1000 g/m 2 ·h at 56 °C. With a high separation factor and butanol flux, the zeolite-filled PDMS MMM would be advantageous for recovering n -butanol from dilute solution at significantly reduced energy input and cost.

Why it matters

OpenAlex reports 51 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Zeolite-filled polydimethylsiloxane (PDMS) mixed matrix membranes (MMMs) were developed for pervaporation separation of n -butanol from dilute butanol–water solution. The effects of zeolite, feed butanol concentration, and temperature were studied. In general, the butanol separation factor increased with increasing the temperature, whereas the fluxes increased with the reducing membrane thickness and increasing feed butanol concentration and temperature. At 47 °C, PDMS MMMs filled with 40 wt % zeolite gave the highest separation factor of 77, which would reduce the energy consumption for butanol recovery from 1.0 wt % butanol by ∼75% to ∼10 MJ/kg butanol using a hybrid pervaporation-distillation process compared to distillation. The zeolite-filled PDMS MMM with a thickness of 10 μm would have a high butanol flux of 1000 g/m 2 ·h at 56 °C. With a high separation factor and butanol flux, the zeolite-filled PDMS MMM would be advantageous for recovering n -butanol from dilute solution at significantly reduced energy input and cost.

Key concepts: Pervaporation, Butanol, Zeolite, n-Butanol, Polydimethylsiloxane, Membrane, Distillation, Chemical engineering

Related papers

Back to paper searchBrowse research topicsOriginal source
High-Performance n-Butanol Recovery from Aqueous Solution by Pervaporation with a PDMS Mixed Matrix Membrane Filled with Zeolite — Research Paper | ScholarLens