Research on Behavior of Iron in the Zinc Sulfide Pressure Leaching Process

Shuchen Qin, Kaixi Jiang, Haibei Wang, Bangsheng Zhang, Yufang Wang, Xuedong Zhang

Open full text 28 citations

Abstract

Dissolved iron exerts significant effects on mineral leaching, impurity removal, and solution purification in the zinc hydrometallurgy process. To date, iron oxidation and migration behaviors are yet to be fully understood and further research on effective regulation mechanisms of iron is required. In this paper, zinc sulfide concentrate was used as the research object. The behaviors of both Zn and Fe during pressure leaching were investigated for varying temperature, acid addition, and leaching time. At temperature of 100~160 °C, H2SO4/Zn ratio of 0.9:1–1.25:1, and leaching time of 0.5–2.5 h, the zinc extraction increased with temperature, acidity and leaching time. The iron extraction, however, varied differently with increasing temperature, acidity and leaching time: (A) it increased with temperature to 150 °C and then decreased at higher temperature, and (B) displayed an initial increase followed by a decrease with respect to the leaching time. Based on the characteristics of the residue phase, chemical phase analysis was used to analyze the residue in detail. The extent of dissolution of iron-containing minerals and the extent of precipitation of ferric ions during the leaching process were quantitatively calculated.

Open-access reader

About this research paper

What this paper is about

Dissolved iron exerts significant effects on mineral leaching, impurity removal, and solution purification in the zinc hydrometallurgy process. To date, iron oxidation and migration behaviors are yet to be fully understood and further research on effective regulation mechanisms of iron is required. In this paper, zinc sulfide concentrate was used as the research object. The behaviors of both Zn and Fe during pressure leaching were investigated for varying temperature, acid addition, and leaching time. At temperature of 100~160 °C, H2SO4/Zn ratio of 0.9:1–1.25:1, and leaching time of 0.5–2.5 h, the zinc extraction increased with temperature, acidity and leaching time. The iron extraction, however, varied differently with increasing temperature, acidity and leaching time: (A) it increased with temperature to 150 °C and then decreased at higher temperature, and (B) displayed an initial increase followed by a decrease with respect to the leaching time. Based on the characteristics of the residue phase, chemical phase analysis was used to analyze the residue in detail. The extent of dissolution of iron-containing minerals and the extent of precipitation of ferric ions during the leaching process were quantitatively calculated.

Why it matters

OpenAlex reports 28 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Dissolved iron exerts significant effects on mineral leaching, impurity removal, and solution purification in the zinc hydrometallurgy process. To date, iron oxidation and migration behaviors are yet to be fully understood and further research on effective regulation mechanisms of iron is required. In this paper, zinc sulfide concentrate was used as the research object. The behaviors of both Zn and Fe during pressure leaching were investigated for varying temperature, acid addition, and leaching time. At temperature of 100~160 °C, H2SO4/Zn ratio of 0.9:1–1.25:1, and leaching time of 0.5–2.5 h, the zinc extraction increased with temperature, acidity and leaching time. The iron extraction, however, varied differently with increasing temperature, acidity and leaching time: (A) it increased with temperature to 150 °C and then decreased at higher temperature, and (B) displayed an initial increase followed by a decrease with respect to the leaching time. Based on the characteristics of the residue phase, chemical phase analysis was used to analyze the residue in detail. The extent of dissolution of iron-containing minerals and the extent of precipitation of ferric ions during the leaching process were quantitatively calculated.

Key concepts: Leaching (pedology), Dissolution, Zinc, Chemistry, Sulfide, Hydrometallurgy, FERRIC IRON, Ferric

Related papers

Back to paper searchBrowse research topicsOriginal source
Research on Behavior of Iron in the Zinc Sulfide Pressure Leaching Process — Research Paper | ScholarLens