2020•Physica ScriptaRequires access

Thermal desorption of hydrogen isotopes from the JET Be plasma facing components

Lı̅ga Avotiņa, Ionut Jepu, Aleksandra Wanda BARON-WIECHEĆ, Michal Kresina, A. Widdowson, JET contributors

Open publisher page 6 citations

Abstract

Understanding of fuel retention and release processes from materials for ITER (International Thermonuclear Experimental Reactor) is important from fundamental and technological aspects. Detailed information regarding fuel retention and release characteristics will allow global fuel inventories to be estimated in fusion devices as well as indicate the requirements for development detritiation methods and the re-use of tritium. Selected beryllium (Be) tiles were extracted from the JET vacuum vessel after each experimental campaign period with the ITER-like wall (ILW); so called ILW1 (2011–2012), ILW2 (2013–2014) and ILW3 (2015–2016). Desorption of hydrogen isotopes of samples taken from the inner wall guard limiter (IWGL), outer poloidal limiter (OPL) and dump plate (DP) tiles were analysed by means of thermal desorption spectrometry (TDS). The results presented compare data across ILW1, ILW2 and ILW3 and show the long term trends of fuel retention in Be limiter tiles. For all three campaigns the level of retention correlates with erosion and deposition that takes place during plasma operations Deuterium retention varies from 0.01–1 × 10 18 atoms cm –2 . Deuterium release takes place in several stages, related to different types of traps which can be within the co-deposit layer and/or below the surface in the Be bulk, with the main release stages around 700–760, 850–900 and 1020 K. The level of tritium in Be was found to be 10 4 times lower than deuterium for ILW campaigns 1–3.

About this research paper

What this paper is about

Understanding of fuel retention and release processes from materials for ITER (International Thermonuclear Experimental Reactor) is important from fundamental and technological aspects. Detailed information regarding fuel retention and release characteristics will allow global fuel inventories to be estimated in fusion devices as well as indicate the requirements for development detritiation methods and the re-use of tritium. Selected beryllium (Be) tiles were extracted from the JET vacuum vessel after each experimental campaign period with the ITER-like wall (ILW); so called ILW1 (2011–2012), ILW2 (2013–2014) and ILW3 (2015–2016). Desorption of hydrogen isotopes of samples taken from the inner wall guard limiter (IWGL), outer poloidal limiter (OPL) and dump plate (DP) tiles were analysed by means of thermal desorption spectrometry (TDS). The results presented compare data across ILW1, ILW2 and ILW3 and show the long term trends of fuel retention in Be limiter tiles. For all three campaigns the level of retention correlates with erosion and deposition that takes place during plasma operations Deuterium retention varies from 0.01–1 × 10 18 atoms cm –2 . Deuterium release takes place in several stages, related to different types of traps which can be within the co-deposit layer and/or below the surface in the Be bulk, with the main release stages around 700–760, 850–900 and 1020 K. The level of tritium in Be was found to be 10 4 times lower than deuterium for ILW campaigns 1–3.

Why it matters

OpenAlex reports 6 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Understanding of fuel retention and release processes from materials for ITER (International Thermonuclear Experimental Reactor) is important from fundamental and technological aspects. Detailed information regarding fuel retention and release characteristics will allow global fuel inventories to be estimated in fusion devices as well as indicate the requirements for development detritiation methods and the re-use of tritium. Selected beryllium (Be) tiles were extracted from the JET vacuum vessel after each experimental campaign period with the ITER-like wall (ILW); so called ILW1 (2011–2012), ILW2 (2013–2014) and ILW3 (2015–2016). Desorption of hydrogen isotopes of samples taken from the inner wall guard limiter (IWGL), outer poloidal limiter (OPL) and dump plate (DP) tiles were analysed by means of thermal desorption spectrometry (TDS). The results presented compare data across ILW1, ILW2 and ILW3 and show the long term trends of fuel retention in Be limiter tiles. For all three campaigns the level of retention correlates with erosion and deposition that takes place during plasma operations Deuterium retention varies from 0.01–1 × 10 18 atoms cm –2 . Deuterium release takes place in several stages, related to different types of traps which can be within the co-deposit layer and/or below the surface in the Be bulk, with the main release stages around 700–760, 850–900 and 1020 K. The level of tritium in Be was found to be 10 4 times lower than deuterium for ILW campaigns 1–3.

Key concepts: Jet (fluid), Hydrogen, Desorption, Plasma, Hydrogen isotope, Thermal desorption, Isotope, Materials science

Related papers

Back to paper searchBrowse research topicsOriginal source
Thermal desorption of hydrogen isotopes from the JET Be plasma facing components — Research Paper | ScholarLens