Effects of Temperature on the Tribological Properties of NM600 under Sliding Wear
Yingchao Pei, Dianxiu Xia, Shouren Wang, Liang Cong, Xuelin Wang, Dongyue Wang
Abstract
Open-access reader
Yingchao Pei, Dianxiu Xia, Shouren Wang, Liang Cong, Xuelin Wang, Dongyue Wang
Abstract
Open-access reader
An investigation on the tribological properties of GCr15 sliding against NM600 was carried out using a high-temperature friction and wear tester. As the temperature rose from room temperature to 300 °C, the average friction coefficient of NM600 increased rapidly, then decreased rapidly, and then became stable. The wear volume and specific wear rate of NM600 increased rapidly, then decreased rapidly, and then increased slowly. The wear mechanism and matrix properties of the tested steel at different temperatures are the main reasons for the above results. At 20-50 °C, the main wear mechanism was adhesive wear, fatigue wear, and abrasive wear. At 100-150 ℃, the wear mechanism was mainly adhesive wear, fatigue wear, abrasive wear, and oxidation wear. At 200-300 °C, the wear mechanism was mainly oxidation wear and abrasive wear.
OpenAlex reports 16 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
An investigation on the tribological properties of GCr15 sliding against NM600 was carried out using a high-temperature friction and wear tester. As the temperature rose from room temperature to 300 °C, the average friction coefficient of NM600 increased rapidly, then decreased rapidly, and then became stable. The wear volume and specific wear rate of NM600 increased rapidly, then decreased rapidly, and then increased slowly. The wear mechanism and matrix properties of the tested steel at different temperatures are the main reasons for the above results. At 20-50 °C, the main wear mechanism was adhesive wear, fatigue wear, and abrasive wear. At 100-150 ℃, the wear mechanism was mainly adhesive wear, fatigue wear, abrasive wear, and oxidation wear. At 200-300 °C, the wear mechanism was mainly oxidation wear and abrasive wear.
Key concepts: Tribology, Materials science, Composite material