Defluoridation of water through the transformation of octacalcium phosphate into fluorapatite
Alfredo Idini, Elisabetta Dore, Dario Fancello, Franco Frau
Abstract
Open-access reader
Alfredo Idini, Elisabetta Dore, Dario Fancello, Franco Frau
Abstract
Open-access reader
The consumption of water with fluoride concentration higher than 1.5 mg/L (WHO recommended limit) is recognized to cause serious diseases, and fluoride removal from natural contaminated waters is a health priority for more than 260 million people worldwide. The octacalcium phosphate (OCP), a mineralogical precursor of bio-apatite, is here tested as a fluoride remover. A new two-step method for the synthesis of OCP is proposed: 1) synthesis of brushite from calcium carbonate and phosphoric acid; 2) subsequent hydrolysis of brushite. Fluoride removal experiments are performed in batch-mode using different initial concentrations of fluoride (from 40 to 140 mg/L) and reaction times. Most of fluoride is removed within the first 2 h of all experiments, and the drinkable limit of 1.5 mg/L is reached within a minimum of 3 h for an initial fluoride concentration of 40 mg/L. The experimental fluoride removal capacity of OCP is 25.7 mg/g, and 4 g of OCP can effectively treat 1 L of water with fluoride concentration up to 50 times higher than the drinking limit of 1.5 mg/L. XRD and chemical characterization of the solid phases, before and after the removal experiments, indicate that OCP transforms into fluorapatite (FAP) uptaking fluoride from solution.
OpenAlex reports 13 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The consumption of water with fluoride concentration higher than 1.5 mg/L (WHO recommended limit) is recognized to cause serious diseases, and fluoride removal from natural contaminated waters is a health priority for more than 260 million people worldwide. The octacalcium phosphate (OCP), a mineralogical precursor of bio-apatite, is here tested as a fluoride remover. A new two-step method for the synthesis of OCP is proposed: 1) synthesis of brushite from calcium carbonate and phosphoric acid; 2) subsequent hydrolysis of brushite. Fluoride removal experiments are performed in batch-mode using different initial concentrations of fluoride (from 40 to 140 mg/L) and reaction times. Most of fluoride is removed within the first 2 h of all experiments, and the drinkable limit of 1.5 mg/L is reached within a minimum of 3 h for an initial fluoride concentration of 40 mg/L. The experimental fluoride removal capacity of OCP is 25.7 mg/g, and 4 g of OCP can effectively treat 1 L of water with fluoride concentration up to 50 times higher than the drinking limit of 1.5 mg/L. XRD and chemical characterization of the solid phases, before and after the removal experiments, indicate that OCP transforms into fluorapatite (FAP) uptaking fluoride from solution.
Key concepts: Fluorapatite, Fluoride, Octacalcium phosphate, Brushite, Apatite, Phosphoric acid, Chemistry, Nuclear chemistry