Study on the Interaction between Galena and Sphalerite During Grinding Based on the Migration of Surface Components
Bo Huang, Hao Lai, Jiushuai Deng, Hongxiang Xu, Guixia Fan
Abstract
Bo Huang, Hao Lai, Jiushuai Deng, Hongxiang Xu, Guixia Fan
Abstract
In Pb-Zn ore flotation, unintentional activation of sphalerite often leads to difficult separation of Pb and Zn minerals, during which grinding plays a key role in unintentional activation. Therefore, the aim of this study was to evaluate the surface component changes of two different mineral particles and to propose the interaction between galena and sphalerite during mixed grinding using time-of-flight secondary ion mass spectrometry (ToF-SIMS). The results show that after mixed grinding of the galena and sphalerite, the Pb content on the sphalerite surface increased with the decrease of Zn and Fe contents on the sphalerite surface. The lead ions from galena were obviously absorbed onto the sphalerite surface, while the zinc and iron ions from sphalerite were not obviously migrated to the galena surface. Principal component analysis (PCA) of a dataset composed of 206 positive ion peaks of galena and sphalerite indicates that the surface components of galena and sphalerite migrated from either side to different degrees. This study successfully identified an important factor for unintentional activation of lead and zinc minerals during flotation: homogenization of surface components of different minerals during grinding.
OpenAlex reports 22 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
In Pb-Zn ore flotation, unintentional activation of sphalerite often leads to difficult separation of Pb and Zn minerals, during which grinding plays a key role in unintentional activation. Therefore, the aim of this study was to evaluate the surface component changes of two different mineral particles and to propose the interaction between galena and sphalerite during mixed grinding using time-of-flight secondary ion mass spectrometry (ToF-SIMS). The results show that after mixed grinding of the galena and sphalerite, the Pb content on the sphalerite surface increased with the decrease of Zn and Fe contents on the sphalerite surface. The lead ions from galena were obviously absorbed onto the sphalerite surface, while the zinc and iron ions from sphalerite were not obviously migrated to the galena surface. Principal component analysis (PCA) of a dataset composed of 206 positive ion peaks of galena and sphalerite indicates that the surface components of galena and sphalerite migrated from either side to different degrees. This study successfully identified an important factor for unintentional activation of lead and zinc minerals during flotation: homogenization of surface components of different minerals during grinding.
Key concepts: Sphalerite, Galena, Grinding, Zinc, Metallurgy, Mineral, Secondary ion mass spectrometry, Chemistry