Fibers are materials with advantageous properties such as lightweight material properties, has small pore size, and has high surface area, porosity,and permeability. An easy and simple method to prepare fibers is electrospinning. Using this method poly(methyl methacrylate) (PMMA) fibers were prepared. Several parameters include polymer concentration, solution flow rate, the distance of the nozzle tip to the collector, and the applied voltage were investigated to control the morphology, structure, and diameter of PMMA fibers. The Optimal electrospinning conditions for PMMA fibers production were a PMMA concentration is 8% (w/v), a power supply voltage is 20 kV, a distance of the tip of the nozzle to the ground collector is 15 cm, and a flow rate is 0.004 mL/min. The diameter distribution and morphology of the fibers were determined and characterized by Optical Microscopy and Scanning Electron Microscope (SEM), which showed that the produced fiber had an average diameter of 1.4925 µm, the contact angle of fiber PMMA is 125.307o and the spreading time of fibers PMMA is about 360 minutes

About this research paper

What this paper is about

Fibers are materials with advantageous properties such as lightweight material properties, has small pore size, and has high surface area, porosity,and permeability. An easy and simple method to prepare fibers is electrospinning. Using this method poly(methyl methacrylate) (PMMA) fibers were prepared. Several parameters include polymer concentration, solution flow rate, the distance of the nozzle tip to the collector, and the applied voltage were investigated to control the morphology, structure, and diameter of PMMA fibers. The Optimal electrospinning conditions for PMMA fibers production were a PMMA concentration is 8% (w/v), a power supply voltage is 20 kV, a distance of the tip of the nozzle to the ground collector is 15 cm, and a flow rate is 0.004 mL/min. The diameter distribution and morphology of the fibers were determined and characterized by Optical Microscopy and Scanning Electron Microscope (SEM), which showed that the produced fiber had an average diameter of 1.4925 µm, the contact angle of fiber PMMA is 125.307o and the spreading time of fibers PMMA is about 360 minutes

Why it matters

OpenAlex reports 3 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Fibers are materials with advantageous properties such as lightweight material properties, has small pore size, and has high surface area, porosity,and permeability. An easy and simple method to prepare fibers is electrospinning. Using this method poly(methyl methacrylate) (PMMA) fibers were prepared. Several parameters include polymer concentration, solution flow rate, the distance of the nozzle tip to the collector, and the applied voltage were investigated to control the morphology, structure, and diameter of PMMA fibers. The Optimal electrospinning conditions for PMMA fibers production were a PMMA concentration is 8% (w/v), a power supply voltage is 20 kV, a distance of the tip of the nozzle to the ground collector is 15 cm, and a flow rate is 0.004 mL/min. The diameter distribution and morphology of the fibers were determined and characterized by Optical Microscopy and Scanning Electron Microscope (SEM), which showed that the produced fiber had an average diameter of 1.4925 µm, the contact angle of fiber PMMA is 125.307o and the spreading time of fibers PMMA is about 360 minutes

Key concepts: Materials science, Electrospinning, Methyl methacrylate, Scanning electron microscope, Composite material, Poly(methyl methacrylate), Porosity, Fiber

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation and Characterization of Poly(Methyl Methacrylate) (PMMA) Fibers by Electrospinning — Research Paper | ScholarLens