20162016 International Conference of Asian Union of Magnetics Societies (ICAUMS)Requires access

The Effect of Nd-Cu Addition on the Coercivity of Hot-Deformed Magnet Prepared with HDDR Powder

Haihang Wang, Renjie Chen, Wenzong Yin, Chaoxiang Jin, Zexuan Wang, Doo Lee, Aru Yan

Open publisher page 0 citations

Abstract

HDDR (hydrogenation disproportionation desorption recombination) has attracted much attention for refining grain size and recycling waste magnets. [1]-[2] However, the coercivity of deformed magnets prepared by HDDR-processed powders (HDDR magnet) are far below the expected value based on their submicron grains, which is attributed to the lack of continuous ultrathin Nd-rich intergranular phase between neighboring Nd2Fe14B matrix grains.[3]

About this research paper

What this paper is about

HDDR (hydrogenation disproportionation desorption recombination) has attracted much attention for refining grain size and recycling waste magnets. [1]-[2] However, the coercivity of deformed magnets prepared by HDDR-processed powders (HDDR magnet) are far below the expected value based on their submicron grains, which is attributed to the lack of continuous ultrathin Nd-rich intergranular phase between neighboring Nd2Fe14B matrix grains.[3]

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

HDDR (hydrogenation disproportionation desorption recombination) has attracted much attention for refining grain size and recycling waste magnets. [1]-[2] However, the coercivity of deformed magnets prepared by HDDR-processed powders (HDDR magnet) are far below the expected value based on their submicron grains, which is attributed to the lack of continuous ultrathin Nd-rich intergranular phase between neighboring Nd2Fe14B matrix grains.[3]

Key concepts: Coercivity, Magnet, Disproportionation, Materials science, Ferromagnetism, Desorption, Analytical Chemistry (journal), Chemical engineering

Related papers

Back to paper searchBrowse research topicsOriginal source
The Effect of Nd-Cu Addition on the Coercivity of Hot-Deformed Magnet Prepared with HDDR Powder — Research Paper | ScholarLens