2018•Advanced Engineering MaterialsRequires access

Microstructure and Properties of C/SiC‐Diamond Composites Prepared by the Combination of CVI and RMI

Jingxin Li, Yongsheng Liu, Beiya Nan, Zhifeng Zhao, Wei Feng, Qing Zhang, Laifei Cheng

Open publisher page 30 citations

Abstract

Diamond modified continuous carbon fiber reinforced silicon carbide (C/SiC‐Diamond) composites are prepared using a combination of chemical vapor infiltration (CVI) and reactive melt infiltration (RMI). The effect of the diamond particle size on the microstructure, mechanical properties, and thermophysical properties of C/SiC‐Diamond composites are investigated. A density of 2.05 g cm−3 is achieved for C/SiC‐Diamond composites impregnated with 1 µm diamond particles. A near twofold enhancement of the thermal conductivity (9–10 W (m K)−1) and thermal diffusion coefficient (5 mm2 s−1) is obtained, compared with continuous carbon fiber reinforced silicon carbide (C/SiC) composites (5–6 W (m · K)−1) prepared by CVI. It is established that the introduction of diamond can improve the thermal conductivity of C/SiC composites and increase the application potential in rocket engines, aerospace vehicles, and brake materials.

About this research paper

What this paper is about

Diamond modified continuous carbon fiber reinforced silicon carbide (C/SiC‐Diamond) composites are prepared using a combination of chemical vapor infiltration (CVI) and reactive melt infiltration (RMI). The effect of the diamond particle size on the microstructure, mechanical properties, and thermophysical properties of C/SiC‐Diamond composites are investigated. A density of 2.05 g cm−3 is achieved for C/SiC‐Diamond composites impregnated with 1 µm diamond particles. A near twofold enhancement of the thermal conductivity (9–10 W (m K)−1) and thermal diffusion coefficient (5 mm2 s−1) is obtained, compared with continuous carbon fiber reinforced silicon carbide (C/SiC) composites (5–6 W (m · K)−1) prepared by CVI. It is established that the introduction of diamond can improve the thermal conductivity of C/SiC composites and increase the application potential in rocket engines, aerospace vehicles, and brake materials.

Why it matters

OpenAlex reports 30 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Diamond modified continuous carbon fiber reinforced silicon carbide (C/SiC‐Diamond) composites are prepared using a combination of chemical vapor infiltration (CVI) and reactive melt infiltration (RMI). The effect of the diamond particle size on the microstructure, mechanical properties, and thermophysical properties of C/SiC‐Diamond composites are investigated. A density of 2.05 g cm−3 is achieved for C/SiC‐Diamond composites impregnated with 1 µm diamond particles. A near twofold enhancement of the thermal conductivity (9–10 W (m K)−1) and thermal diffusion coefficient (5 mm2 s−1) is obtained, compared with continuous carbon fiber reinforced silicon carbide (C/SiC) composites (5–6 W (m · K)−1) prepared by CVI. It is established that the introduction of diamond can improve the thermal conductivity of C/SiC composites and increase the application potential in rocket engines, aerospace vehicles, and brake materials.

Key concepts: Materials science, Diamond, Composite material, Microstructure, Thermal conductivity, Silicon carbide, Chemical vapor infiltration, Ceramic

Related papers

Back to paper searchBrowse research topicsOriginal source
Microstructure and Properties of C/SiC‐Diamond Composites Prepared by the Combination of CVI and RMI — Research Paper | ScholarLens