Microleakage of glass ionomer based restorative materials in primary teeth: An In vitro study
Buket Ayna, Sema Çelenk, Osman Ataş, Emin Caner Tümen, Ersin Uysal, I R Toptanci
Abstract
Buket Ayna, Sema Çelenk, Osman Ataş, Emin Caner Tümen, Ersin Uysal, I R Toptanci
Abstract
AIM: Using AutoCAD, we examined the microleakage of dye at the edges of primary-teeth restorations using three glass ionomer-based restorative materials. MATERIALS AND METHODS: A total of 30 extracted noncarious primary molars were used. Class V cavities were adjusted on the buccal surfaces. The teeth were randomly divided into three groups of 10 teeth each as follows: Group A (Ketac Molar), Group B (Photac Fil), and Group C (Dyract XP). All specimens were stored for 24 h at 37°C in distilled water. The teeth were thermocycled 1000 times between 5°C ± 2°C and 55°C ± 2°C before immersion in 0.5% basic fuchsin for 24 h. Two mesiodistal cuts of each tooth were photographed under a stereomicroscope equipped with a digital camera. The dye-infiltrated surface area was measured. Statistical evaluations were performed by the Kolmogorov-Smirnov test, Levene test, one-way analysis of variance, and Tukey's honestly significant difference test. RESULTS: The mean microleakage ratio differed significantly among the groups (P < 0.05). Group C exhibited a significantly smaller area (P < 0.001) than the other groups. Group A had a nonsignificantly higher mean microleakage value than Group B (P > 0.05). CONCLUSIONS: Polyacid-modified composite resin may be a useful restorative material in primary teeth in terms of minimizing microleakage.
OpenAlex reports 14 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
AIM: Using AutoCAD, we examined the microleakage of dye at the edges of primary-teeth restorations using three glass ionomer-based restorative materials. MATERIALS AND METHODS: A total of 30 extracted noncarious primary molars were used. Class V cavities were adjusted on the buccal surfaces. The teeth were randomly divided into three groups of 10 teeth each as follows: Group A (Ketac Molar), Group B (Photac Fil), and Group C (Dyract XP). All specimens were stored for 24 h at 37°C in distilled water. The teeth were thermocycled 1000 times between 5°C ± 2°C and 55°C ± 2°C before immersion in 0.5% basic fuchsin for 24 h. Two mesiodistal cuts of each tooth were photographed under a stereomicroscope equipped with a digital camera. The dye-infiltrated surface area was measured. Statistical evaluations were performed by the Kolmogorov-Smirnov test, Levene test, one-way analysis of variance, and Tukey's honestly significant difference test. RESULTS: The mean microleakage ratio differed significantly among the groups (P < 0.05). Group C exhibited a significantly smaller area (P < 0.001) than the other groups. Group A had a nonsignificantly higher mean microleakage value than Group B (P > 0.05). CONCLUSIONS: Polyacid-modified composite resin may be a useful restorative material in primary teeth in terms of minimizing microleakage.
Key concepts: Glass ionomer cement, Molar, Dentistry, Stereo microscope, Medicine, Significant difference, Orthodontics, Statistical analysis