In diffusion brazing, a brazing alloy layer thickness introduced into the gap between brazed parts is very small, which hinders the study of the isothermal solidification process. In this work, the isothermal solidification of an Al–Zn alloy is investigated at large volume and mass of the initial liquid that takes part in isothermal solidification. Zinc cylinders are caulked in the holes bored in aluminum cubes. The samples thus assembled are held at 500 ± 10°C for different times. The volume fraction of isothermal solidified crystals has been determined, and the growth rate of isothermal crystals is shown to decrease upon holding. The crystals formed during isothermal solidification width are up to 380 μm and length more than 1 mm. They are observed in the samples that are held more than 2 days. The zinc content in the isothermal solidified crystals corresponds to its mean content in the aluminum solid solution at 490–510°C, according to the Al–Zn phase diagram. The composition of the former liquid that surrounded the crystals during isothermal solidification coincides with the equilibrium composition of the liquid in the Al–Zn system at a temperature of 490–510°C.

About this research paper

What this paper is about

In diffusion brazing, a brazing alloy layer thickness introduced into the gap between brazed parts is very small, which hinders the study of the isothermal solidification process. In this work, the isothermal solidification of an Al–Zn alloy is investigated at large volume and mass of the initial liquid that takes part in isothermal solidification. Zinc cylinders are caulked in the holes bored in aluminum cubes. The samples thus assembled are held at 500 ± 10°C for different times. The volume fraction of isothermal solidified crystals has been determined, and the growth rate of isothermal crystals is shown to decrease upon holding. The crystals formed during isothermal solidification width are up to 380 μm and length more than 1 mm. They are observed in the samples that are held more than 2 days. The zinc content in the isothermal solidified crystals corresponds to its mean content in the aluminum solid solution at 490–510°C, according to the Al–Zn phase diagram. The composition of the former liquid that surrounded the crystals during isothermal solidification coincides with the equilibrium composition of the liquid in the Al–Zn system at a temperature of 490–510°C.

Why it matters

OpenAlex reports 8 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

In diffusion brazing, a brazing alloy layer thickness introduced into the gap between brazed parts is very small, which hinders the study of the isothermal solidification process. In this work, the isothermal solidification of an Al–Zn alloy is investigated at large volume and mass of the initial liquid that takes part in isothermal solidification. Zinc cylinders are caulked in the holes bored in aluminum cubes. The samples thus assembled are held at 500 ± 10°C for different times. The volume fraction of isothermal solidified crystals has been determined, and the growth rate of isothermal crystals is shown to decrease upon holding. The crystals formed during isothermal solidification width are up to 380 μm and length more than 1 mm. They are observed in the samples that are held more than 2 days. The zinc content in the isothermal solidified crystals corresponds to its mean content in the aluminum solid solution at 490–510°C, according to the Al–Zn phase diagram. The composition of the former liquid that surrounded the crystals during isothermal solidification coincides with the equilibrium composition of the liquid in the Al–Zn system at a temperature of 490–510°C.

Key concepts: Isothermal process, Materials science, Alloy, Volume fraction, Diffusion, Brazing, Metallurgy, Aluminium

Related papers

Back to paper searchBrowse research topicsOriginal source
Isothermal Solidification of an Al–Zn Alloy — Research Paper | ScholarLens