This research was undertaken to study the effect of adding silver nitrate (AgNO3) during leaching of gold ore for Au recovery. Its focus is to obtain the weight of Au in feed and concentrate, the effect of AgNO3 on Au recovery, theconcentration of AgNO3 that led to optimum recovery, and the weight of bullion and Au content in bullion. This research was conducted using quantitative descriptive method with experimental technique and the research steps include the following: 1) rock and treatment plant preparation, 2) tests with variable AgNO3 concentrations, 3) analysis feed and concentrate samples using atomic absorption spectroscopy (AAS), 4) measurement of concentrate density, 5) burning of activated carbon to get the bullion, and 6) weighing bullion and Au content. There was increase Au recovery from 12.57% to 36.15%. On addition of 0 to 4 gram of AgNO3, whereby highest recovery was obtained on the addition of 4 g of AgNO3 concentration to 150 kg of feed.
OpenAlex reports 5 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
This research was undertaken to study the effect of adding silver nitrate (AgNO3) during leaching of gold ore for Au recovery. Its focus is to obtain the weight of Au in feed and concentrate, the effect of AgNO3 on Au recovery, theconcentration of AgNO3 that led to optimum recovery, and the weight of bullion and Au content in bullion. This research was conducted using quantitative descriptive method with experimental technique and the research steps include the following: 1) rock and treatment plant preparation, 2) tests with variable AgNO3 concentrations, 3) analysis feed and concentrate samples using atomic absorption spectroscopy (AAS), 4) measurement of concentrate density, 5) burning of activated carbon to get the bullion, and 6) weighing bullion and Au content. There was increase Au recovery from 12.57% to 36.15%. On addition of 0 to 4 gram of AgNO3, whereby highest recovery was obtained on the addition of 4 g of AgNO3 concentration to 150 kg of feed.
Key concepts: Gold cyanidation, Gold ore, Heap leaching, Metallurgy, Heap (data structure), Leaching (pedology), Materials science, Environmental science