A Transient Finite Element Model to Simulate the Physical Mechanisms of High-speed Wheel/rail Rolling Contact on a Rail Welding Joint
Miao Yu, Weidong Wang, Jinzhao Liu
Abstract
Open-access reader
Miao Yu, Weidong Wang, Jinzhao Liu
Abstract
Open-access reader
In order to study the influences of defective rail welding joints on wheel/rail interaction, a transient finite element model of a high-speed train passing over rail welding joints is presented on the basis of field measurements. Focusing on the physical mechanisms differences of wheel/rail rolling contact on welding joints with varying rail straightness at rolling speeds of up to 400 km/h, this model takes vehicle/track system dynamics and wheel/rail elastic–plastic deformations into account. The defective thermite welding joint with short wave irregularity easily leads to rail nucleus flaw with residual stress. When the running speed is over 250km/h,the maximum value of wheel/rail vertical force at welding joint has a basic trend of a bilinear increase with the increase of running speed and the unevenness of the welding joint. There is a phase difference between the maximum contact force and the peak joint irregularity. When the high-speed railway operation management standard is 250~350km/h, the short wave irregularity at rail welding joint with over 0.3mm straightness should be grinded.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
In order to study the influences of defective rail welding joints on wheel/rail interaction, a transient finite element model of a high-speed train passing over rail welding joints is presented on the basis of field measurements. Focusing on the physical mechanisms differences of wheel/rail rolling contact on welding joints with varying rail straightness at rolling speeds of up to 400 km/h, this model takes vehicle/track system dynamics and wheel/rail elastic–plastic deformations into account. The defective thermite welding joint with short wave irregularity easily leads to rail nucleus flaw with residual stress. When the running speed is over 250km/h,the maximum value of wheel/rail vertical force at welding joint has a basic trend of a bilinear increase with the increase of running speed and the unevenness of the welding joint. There is a phase difference between the maximum contact force and the peak joint irregularity. When the high-speed railway operation management standard is 250~350km/h, the short wave irregularity at rail welding joint with over 0.3mm straightness should be grinded.
Key concepts: Welding, Joint (building), Welding joint, Finite element method, Structural engineering, Transient (computer programming), Track (disk drive), Engineering