2017IOP Conference Series Materials Science and EngineeringOpen access

Properties of concrete containing ground palm oil fuel ash as fine aggregate replacement

Wan Ahmad Saffuan, Khairunisa Muthusamy, Nur Afiqah Mohd Salleh, Norhaiza Nordin

Open full text 23 citations

Abstract

Environmental degradation resulting from increasing sand mining activities and disposal of palm oil fuel ash (POFA), a solid waste generated from palm oil mill needs to be resolved. Thus, the present research investigates the effect of ground palm oil fuel ash as partial fine aggregate replacement on workability, compressive and flexural strength of concrete. Five mixtures of concrete containing POFA as partial sand replacement designed with 0%, 10%, 20%, 30% and 40% of POFA by the weight of sand were used in this experimental work. The cube and beam specimens were casted and water cured up to 28 days before subjected to compressive strength and flexural strength testing respectively. Finding shows that concrete workability reduces as the amount of POFA added become larger. It is worth to note that 10% of POFA is the best amount to be used as partial fine aggregate replacement to produce concrete with enhanced strength.

Open-access reader

About this research paper

What this paper is about

Environmental degradation resulting from increasing sand mining activities and disposal of palm oil fuel ash (POFA), a solid waste generated from palm oil mill needs to be resolved. Thus, the present research investigates the effect of ground palm oil fuel ash as partial fine aggregate replacement on workability, compressive and flexural strength of concrete. Five mixtures of concrete containing POFA as partial sand replacement designed with 0%, 10%, 20%, 30% and 40% of POFA by the weight of sand were used in this experimental work. The cube and beam specimens were casted and water cured up to 28 days before subjected to compressive strength and flexural strength testing respectively. Finding shows that concrete workability reduces as the amount of POFA added become larger. It is worth to note that 10% of POFA is the best amount to be used as partial fine aggregate replacement to produce concrete with enhanced strength.

Why it matters

OpenAlex reports 23 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Environmental degradation resulting from increasing sand mining activities and disposal of palm oil fuel ash (POFA), a solid waste generated from palm oil mill needs to be resolved. Thus, the present research investigates the effect of ground palm oil fuel ash as partial fine aggregate replacement on workability, compressive and flexural strength of concrete. Five mixtures of concrete containing POFA as partial sand replacement designed with 0%, 10%, 20%, 30% and 40% of POFA by the weight of sand were used in this experimental work. The cube and beam specimens were casted and water cured up to 28 days before subjected to compressive strength and flexural strength testing respectively. Finding shows that concrete workability reduces as the amount of POFA added become larger. It is worth to note that 10% of POFA is the best amount to be used as partial fine aggregate replacement to produce concrete with enhanced strength.

Key concepts: Palm oil, Flexural strength, Compressive strength, Aggregate (composite), Materials science, Waste management, Environmental science, Composite material

Related papers

Back to paper searchBrowse research topicsOriginal source
Properties of concrete containing ground palm oil fuel ash as fine aggregate replacement — Research Paper | ScholarLens