Effect of calcination temperature on the structure and catalytic performance of 80Ni20CO/SiO2 catalyst for CO2 methanation
Sherif Abdulbari Ali, K H Ku Hamid, Khairul Nizar Ismail
Abstract
Sherif Abdulbari Ali, K H Ku Hamid, Khairul Nizar Ismail
Abstract
The 80Ni20Co/SiO2 catalysts prepared using co-precipitate and incipient wetness impregnation method were used for production of methane through CO2 methanation reaction between CO and H2 gases. The effect of a range of calcination temperature on the structure and catalytic performance of 80Ni20Co/SiO2 catalyst was investigated using microactivity fixed bed reactor. It was found that the catalyst calcined at 400°C for 4.5 h under air atmosphere has shown the best catalytic performance for CO2 methanation. Characterization of 80Ni20Co/SiO2 catalyst calcined fresh samples was carried out using TPR-H2 analysis, Brunauere Emmette Teller (BET) measurements and X-ray diffraction (XRD. It was observed that calcination temperature influenced the structure, morphology and catalytic performance of the catalysts.
OpenAlex reports 5 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The 80Ni20Co/SiO2 catalysts prepared using co-precipitate and incipient wetness impregnation method were used for production of methane through CO2 methanation reaction between CO and H2 gases. The effect of a range of calcination temperature on the structure and catalytic performance of 80Ni20Co/SiO2 catalyst was investigated using microactivity fixed bed reactor. It was found that the catalyst calcined at 400°C for 4.5 h under air atmosphere has shown the best catalytic performance for CO2 methanation. Characterization of 80Ni20Co/SiO2 catalyst calcined fresh samples was carried out using TPR-H2 analysis, Brunauere Emmette Teller (BET) measurements and X-ray diffraction (XRD. It was observed that calcination temperature influenced the structure, morphology and catalytic performance of the catalysts.
Key concepts: Methanation, Calcination, Catalysis, Incipient wetness impregnation, Materials science, Methane, Atmospheric temperature range, Chemical engineering