Biooxidation of a Refractory Gold Ore: Implications of Whole-Ore Heap Biooxidation
Bo Wei Chen, Jian Sun, He Shang, Biao Wu, Jian Kang Wen
Abstract
Bo Wei Chen, Jian Sun, He Shang, Biao Wu, Jian Kang Wen
Abstract
The Sawayardun Gold Mine, the first Muruntau type gold mine in China, was located in the south Tianshan Mountain, Xinjiang Province. The gold reserve was 127 t with an average gold grade of 2.36 g/t. Due to the high content of arsenic and antimony, the traditional flotation-roasting-cyanidation process was not suitable. The direct cyanidation gold extraction for the raw ore was 44.70 %. Thus, biooxidation experiments in shaker flasks were conducted for this ore. The optimum conditions were obtained as inoculation volume 10 %, initial pH 1.7, pulp density 15 %, temperature 33 °C, leaching time 10 days, with the arsenic oxidation rate of 75.12 %. Then the biooxidation residues were test for gold leaching using NaCN, green gold leaching agent and thiourea. After 24 h leaching rate at pulp density of 33%, gold leaching agent dosage of 2 kg/t ore, the gold extraction for NaCN, green gold leaching agent and thiourea were 91.50 %, 86.23 % and 91.09 %, respectively. The high gold extraction showed a bright future for the whole-ore heap biooxidation of this refractory gold ore.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The Sawayardun Gold Mine, the first Muruntau type gold mine in China, was located in the south Tianshan Mountain, Xinjiang Province. The gold reserve was 127 t with an average gold grade of 2.36 g/t. Due to the high content of arsenic and antimony, the traditional flotation-roasting-cyanidation process was not suitable. The direct cyanidation gold extraction for the raw ore was 44.70 %. Thus, biooxidation experiments in shaker flasks were conducted for this ore. The optimum conditions were obtained as inoculation volume 10 %, initial pH 1.7, pulp density 15 %, temperature 33 °C, leaching time 10 days, with the arsenic oxidation rate of 75.12 %. Then the biooxidation residues were test for gold leaching using NaCN, green gold leaching agent and thiourea. After 24 h leaching rate at pulp density of 33%, gold leaching agent dosage of 2 kg/t ore, the gold extraction for NaCN, green gold leaching agent and thiourea were 91.50 %, 86.23 % and 91.09 %, respectively. The high gold extraction showed a bright future for the whole-ore heap biooxidation of this refractory gold ore.
Key concepts: Gold cyanidation, Gold extraction, Gold ore, Metallurgy, Heap leaching, Leaching (pedology), Arsenopyrite, Arsenic