Thermal shock resistant properties of reaction sintered bauxite-based β-Sialon bonded corundum have been investigated, and the results are compared with those of Al2 O3 based counterpart. It is found they all have very good thermal shock resistance. Their residual strength ratios after one thermal shock cycle at △T =1200℃ and △T = 1350℃ are 61% ~73% and 53% ~65% respectively. Their critical temperature difference (TSR) is 600℃~800℃. TSR parameters are calculated based on thermal expansion, modulus of elasticity,and fracture toughness determined. The reasons for improving TSR of these composite materials are discussed.

About this research paper

What this paper is about

Thermal shock resistant properties of reaction sintered bauxite-based β-Sialon bonded corundum have been investigated, and the results are compared with those of Al2 O3 based counterpart. It is found they all have very good thermal shock resistance. Their residual strength ratios after one thermal shock cycle at △T =1200℃ and △T = 1350℃ are 61% ~73% and 53% ~65% respectively. Their critical temperature difference (TSR) is 600℃~800℃. TSR parameters are calculated based on thermal expansion, modulus of elasticity,and fracture toughness determined. The reasons for improving TSR of these composite materials are discussed.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Thermal shock resistant properties of reaction sintered bauxite-based β-Sialon bonded corundum have been investigated, and the results are compared with those of Al2 O3 based counterpart. It is found they all have very good thermal shock resistance. Their residual strength ratios after one thermal shock cycle at △T =1200℃ and △T = 1350℃ are 61% ~73% and 53% ~65% respectively. Their critical temperature difference (TSR) is 600℃~800℃. TSR parameters are calculated based on thermal expansion, modulus of elasticity,and fracture toughness determined. The reasons for improving TSR of these composite materials are discussed.

Key concepts: Thermal shock, Corundum, Materials science, Sialon, Bauxite, Composite material, Thermal expansion, Residual strength

Related papers

Back to paper searchBrowse research topicsOriginal source
Thermal Shock Resistance of Bauxite-based β-Sialon Bonded Corundum Materials — Research Paper | ScholarLens