Objective: The aim was to evaluate, in vitro, the tensile bond strength to dentin of Scotchbond Universal (SU), All-Bond Universal (AU) and One Coat 7 Universal (OC7) adhesives applied in self-etch mode, after 24 h of storage and after 500,000 loading cycles, using Clearfil SE Bond (SE) as a control. Materials and Methods: The adhesives were applied on the dentin of bovine teeth, followed by the application of a composite resin. Thirty specimens were obtained for each adhesive. Half of the specimens were submitted to cyclic loading for 500,000 cycles. All specimens were submitted to a tensile bond strength test in a universal testing machine at a crosshead speed of 0.5 mm/minute. Results: According to two-way ANOVA and Tukey’s test (α=5%), the interaction between the adhesive and cyclic loading factors was significant (p=0.001). The means followed by the same letter represent no significant difference in the bond strength (MPa) after 24 h: OC7=7.86A (±2.90), SU=6.78AB (±2.03), AU=5.61BC (±2.32), and SE=3.53C (±1.89). After cyclic loading, SE, SU and AU maintained bond strength comparable to 24 h period. There was a significant decrease only for OC7. Conclusion: SU, AU and OC7 had bond strength to dentin comparable to that of SE. Only OC7 had decreased bond strength to dentin after cyclic loading.

Open-access reader

About this research paper

What this paper is about

Objective: The aim was to evaluate, in vitro, the tensile bond strength to dentin of Scotchbond Universal (SU), All-Bond Universal (AU) and One Coat 7 Universal (OC7) adhesives applied in self-etch mode, after 24 h of storage and after 500,000 loading cycles, using Clearfil SE Bond (SE) as a control. Materials and Methods: The adhesives were applied on the dentin of bovine teeth, followed by the application of a composite resin. Thirty specimens were obtained for each adhesive. Half of the specimens were submitted to cyclic loading for 500,000 cycles. All specimens were submitted to a tensile bond strength test in a universal testing machine at a crosshead speed of 0.5 mm/minute. Results: According to two-way ANOVA and Tukey’s test (α=5%), the interaction between the adhesive and cyclic loading factors was significant (p=0.001). The means followed by the same letter represent no significant difference in the bond strength (MPa) after 24 h: OC7=7.86A (±2.90), SU=6.78AB (±2.03), AU=5.61BC (±2.32), and SE=3.53C (±1.89). After cyclic loading, SE, SU and AU maintained bond strength comparable to 24 h period. There was a significant decrease only for OC7. Conclusion: SU, AU and OC7 had bond strength to dentin comparable to that of SE. Only OC7 had decreased bond strength to dentin after cyclic loading.

Why it matters

OpenAlex reports 22 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Objective: The aim was to evaluate, in vitro, the tensile bond strength to dentin of Scotchbond Universal (SU), All-Bond Universal (AU) and One Coat 7 Universal (OC7) adhesives applied in self-etch mode, after 24 h of storage and after 500,000 loading cycles, using Clearfil SE Bond (SE) as a control. Materials and Methods: The adhesives were applied on the dentin of bovine teeth, followed by the application of a composite resin. Thirty specimens were obtained for each adhesive. Half of the specimens were submitted to cyclic loading for 500,000 cycles. All specimens were submitted to a tensile bond strength test in a universal testing machine at a crosshead speed of 0.5 mm/minute. Results: According to two-way ANOVA and Tukey’s test (α=5%), the interaction between the adhesive and cyclic loading factors was significant (p=0.001). The means followed by the same letter represent no significant difference in the bond strength (MPa) after 24 h: OC7=7.86A (±2.90), SU=6.78AB (±2.03), AU=5.61BC (±2.32), and SE=3.53C (±1.89). After cyclic loading, SE, SU and AU maintained bond strength comparable to 24 h period. There was a significant decrease only for OC7. Conclusion: SU, AU and OC7 had bond strength to dentin comparable to that of SE. Only OC7 had decreased bond strength to dentin after cyclic loading.

Key concepts: Bond strength, Crosshead, Dentin, Adhesive, Universal testing machine, Materials science, Ultimate tensile strength, Composite material

Related papers

Back to paper searchBrowse research topicsOriginal source
Bond Capability of Universal Adhesive Systems to Dentin in Self-etch Mode after Short-term Storage and Cyclic Loading — Research Paper | ScholarLens