2017Dental Press Journal of OrthodonticsOpen access

Prototype to measure bracket debonding force in vivo

Jéssika Lagni Tonus, Fernanda Borguetti Manfroi, Gilberto Antônio Borges, Eduardo Correa Grigolo, Sérgio Helegda, Ana Maria Spohr

Open full text 5 citations

Abstract

INTRODUCTION: Material biodegradation that occurs in the mouth may interfere in the bonding strength between the bracket and the enamel, causing lower bond strength values in vivo, in comparison with in vitro studies. OBJECTIVE: To develop a prototype to measure bracket debonding force in vivo and to evaluate, in vitro, the bond strength obtained with the prototype. METHODS: A original plier (3M Unitek) was modified by adding one strain gauge directly connected to its claw. An electronic circuit performed the reading of the strain gauge, and the software installed in a computer recorded the values of the bracket debonding force, in kgf. Orthodontic brackets were bonded to the facial surface of 30 bovine incisors with adhesive materials. In Group 1 (n = 15), debonding was carried out with the prototype, while tensile bond strength testing was performed in Group 2 (n = 15). A universal testing machine was used for the second group. The adhesive remnant index (ARI) was recorded. RESULTS: According to Student's t test (α = 0.05), Group 1 (2.96 MPa) and Group 2 (3.08 MPa) were not significantly different. ARI score of 3 was predominant in the two groups. CONCLUSION: The prototype proved to be reliable for obtaining in vivo bond strength values for orthodontic brackets.

Open-access reader

About this research paper

What this paper is about

INTRODUCTION: Material biodegradation that occurs in the mouth may interfere in the bonding strength between the bracket and the enamel, causing lower bond strength values in vivo, in comparison with in vitro studies. OBJECTIVE: To develop a prototype to measure bracket debonding force in vivo and to evaluate, in vitro, the bond strength obtained with the prototype. METHODS: A original plier (3M Unitek) was modified by adding one strain gauge directly connected to its claw. An electronic circuit performed the reading of the strain gauge, and the software installed in a computer recorded the values of the bracket debonding force, in kgf. Orthodontic brackets were bonded to the facial surface of 30 bovine incisors with adhesive materials. In Group 1 (n = 15), debonding was carried out with the prototype, while tensile bond strength testing was performed in Group 2 (n = 15). A universal testing machine was used for the second group. The adhesive remnant index (ARI) was recorded. RESULTS: According to Student's t test (α = 0.05), Group 1 (2.96 MPa) and Group 2 (3.08 MPa) were not significantly different. ARI score of 3 was predominant in the two groups. CONCLUSION: The prototype proved to be reliable for obtaining in vivo bond strength values for orthodontic brackets.

Why it matters

OpenAlex reports 5 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

INTRODUCTION: Material biodegradation that occurs in the mouth may interfere in the bonding strength between the bracket and the enamel, causing lower bond strength values in vivo, in comparison with in vitro studies. OBJECTIVE: To develop a prototype to measure bracket debonding force in vivo and to evaluate, in vitro, the bond strength obtained with the prototype. METHODS: A original plier (3M Unitek) was modified by adding one strain gauge directly connected to its claw. An electronic circuit performed the reading of the strain gauge, and the software installed in a computer recorded the values of the bracket debonding force, in kgf. Orthodontic brackets were bonded to the facial surface of 30 bovine incisors with adhesive materials. In Group 1 (n = 15), debonding was carried out with the prototype, while tensile bond strength testing was performed in Group 2 (n = 15). A universal testing machine was used for the second group. The adhesive remnant index (ARI) was recorded. RESULTS: According to Student's t test (α = 0.05), Group 1 (2.96 MPa) and Group 2 (3.08 MPa) were not significantly different. ARI score of 3 was predominant in the two groups. CONCLUSION: The prototype proved to be reliable for obtaining in vivo bond strength values for orthodontic brackets.

Key concepts: Bracket, Measure (data warehouse), In vivo, Computer science, Structural engineering, Engineering, Biology, Data mining

Related papers

Back to paper searchBrowse research topicsOriginal source
Prototype to measure bracket debonding force in vivo — Research Paper | ScholarLens