The Degradation of Lignin, Cellulose, and Hemicellulose in Kenaf Bast Under Different Pressures Using Steam Explosion Treatment

Wei Jiang, Guangting Han, Chengfeng Zhou, Shengchuan Gao, Yuanming Zhang, Minghua Li, Ying Gong, Brian K. Via

Open publisher page 34 citations

Abstract

The study of the main chemical composition degradation, especially cellulose degradation at high temperatures and within high moisture environments, provides important information that can guide biomass processing using steam explosion (STEX) and other similar treatments. In this paper, kenaf bast was treated using STEX at pressures of 0.5, 1.0, and 1.5 MPa. The chemical composition change and the infrared spectra were investigated. The crystalline index and degree of polymerization of kenaf cellulose were also quantified. It was found that pectin and hemicellulose could be easily degraded with the STEX treatment, while lignin only exhibited slight decomposition; cellulose degraded at 1.5 MPa STEX treatment on the kenaf. Research also indicates that cellulose with a low molecular weight can be removed with a low-pressure STEX treatment. By coupling STEX with chemical degumming process, the high-quality kenaf fiber with 7.12% residue gum content and 134.5 Nm fineness can be obtained.

About this research paper

What this paper is about

The study of the main chemical composition degradation, especially cellulose degradation at high temperatures and within high moisture environments, provides important information that can guide biomass processing using steam explosion (STEX) and other similar treatments. In this paper, kenaf bast was treated using STEX at pressures of 0.5, 1.0, and 1.5 MPa. The chemical composition change and the infrared spectra were investigated. The crystalline index and degree of polymerization of kenaf cellulose were also quantified. It was found that pectin and hemicellulose could be easily degraded with the STEX treatment, while lignin only exhibited slight decomposition; cellulose degraded at 1.5 MPa STEX treatment on the kenaf. Research also indicates that cellulose with a low molecular weight can be removed with a low-pressure STEX treatment. By coupling STEX with chemical degumming process, the high-quality kenaf fiber with 7.12% residue gum content and 134.5 Nm fineness can be obtained.

Why it matters

OpenAlex reports 34 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The study of the main chemical composition degradation, especially cellulose degradation at high temperatures and within high moisture environments, provides important information that can guide biomass processing using steam explosion (STEX) and other similar treatments. In this paper, kenaf bast was treated using STEX at pressures of 0.5, 1.0, and 1.5 MPa. The chemical composition change and the infrared spectra were investigated. The crystalline index and degree of polymerization of kenaf cellulose were also quantified. It was found that pectin and hemicellulose could be easily degraded with the STEX treatment, while lignin only exhibited slight decomposition; cellulose degraded at 1.5 MPa STEX treatment on the kenaf. Research also indicates that cellulose with a low molecular weight can be removed with a low-pressure STEX treatment. By coupling STEX with chemical degumming process, the high-quality kenaf fiber with 7.12% residue gum content and 134.5 Nm fineness can be obtained.

Key concepts: Hemicellulose, Kenaf, Cellulose, Lignin, Steam explosion, Chemistry, Bast fibre, Chemical composition

Related papers

Back to paper searchBrowse research topicsOriginal source
The Degradation of Lignin, Cellulose, and Hemicellulose in Kenaf Bast Under Different Pressures Using Steam Explosion Treatment — Research Paper | ScholarLens