2016Journal of Wood Chemistry and TechnologyRequires access

Activated carbon from cherry stones by chemical activation: Influence of the impregnation method on porous structure

José M. González‐Domínguez, María Alexandre-Franco, Carmen Fernández-González, Alejandro Ansón‐Casaos, V. Gómez-Serrano

Open publisher page 22 citations

Abstract

Cherry stones are utilized as a precursor for the preparation of activated carbons by chemical activation with phosphoric acid (H3PO4). The activation process typically consists of successive impregnation, carbonization, and washing stages. Here, several impregnation variables are comprehensively studied, including H3PO4 concentration, number of soaking steps, H3PO4 recycling, washing of the impregnated material, and previous semi-carbonization. The choice of a suitable impregnation methodology opens up additional possibilities for the preparation of a wide variety of activated carbons with high yields and tailored porous structures. Microporous activated carbons with specific surface areas of ∼800 m2 g−1 are produced, in which > 60% of the total pore volume is due to micropores. High surface areas of ∼1500 m2 g−1 can be also developed, with micropore volumes being a 26% of the total pore volume. Interestingly, using the same amount of H3PO4, either carbons with surface areas of 791 and 337 m2 g−1 or only one carbon with a surface area of 640 m2 g−1 can be prepared. The pore volumes range very widely between 0.07–0.55, 0.01–0.90, and 0.09–0.79 cm3 g−1 for micropores, mesopores, and macropores, respectively.

About this research paper

What this paper is about

Cherry stones are utilized as a precursor for the preparation of activated carbons by chemical activation with phosphoric acid (H3PO4). The activation process typically consists of successive impregnation, carbonization, and washing stages. Here, several impregnation variables are comprehensively studied, including H3PO4 concentration, number of soaking steps, H3PO4 recycling, washing of the impregnated material, and previous semi-carbonization. The choice of a suitable impregnation methodology opens up additional possibilities for the preparation of a wide variety of activated carbons with high yields and tailored porous structures. Microporous activated carbons with specific surface areas of ∼800 m2 g−1 are produced, in which > 60% of the total pore volume is due to micropores. High surface areas of ∼1500 m2 g−1 can be also developed, with micropore volumes being a 26% of the total pore volume. Interestingly, using the same amount of H3PO4, either carbons with surface areas of 791 and 337 m2 g−1 or only one carbon with a surface area of 640 m2 g−1 can be prepared. The pore volumes range very widely between 0.07–0.55, 0.01–0.90, and 0.09–0.79 cm3 g−1 for micropores, mesopores, and macropores, respectively.

Why it matters

OpenAlex reports 22 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Cherry stones are utilized as a precursor for the preparation of activated carbons by chemical activation with phosphoric acid (H3PO4). The activation process typically consists of successive impregnation, carbonization, and washing stages. Here, several impregnation variables are comprehensively studied, including H3PO4 concentration, number of soaking steps, H3PO4 recycling, washing of the impregnated material, and previous semi-carbonization. The choice of a suitable impregnation methodology opens up additional possibilities for the preparation of a wide variety of activated carbons with high yields and tailored porous structures. Microporous activated carbons with specific surface areas of ∼800 m2 g−1 are produced, in which > 60% of the total pore volume is due to micropores. High surface areas of ∼1500 m2 g−1 can be also developed, with micropore volumes being a 26% of the total pore volume. Interestingly, using the same amount of H3PO4, either carbons with surface areas of 791 and 337 m2 g−1 or only one carbon with a surface area of 640 m2 g−1 can be prepared. The pore volumes range very widely between 0.07–0.55, 0.01–0.90, and 0.09–0.79 cm3 g−1 for micropores, mesopores, and macropores, respectively.

Key concepts: Carbonization, Microporous material, Phosphoric acid, Activated carbon, Mesoporous material, Macropore, Chemistry, Porosity

Related papers

Back to paper searchBrowse research topicsOriginal source
Activated carbon from cherry stones by chemical activation: Influence of the impregnation method on porous structure — Research Paper | ScholarLens