2008Guisuanyan tongbaoRequires access

Preparation of Mixed Conducting Membrane SrFe_(0.7)Cu_(0.3)O_(3-δ) by Sol-Gel Method

Lin Wei-ming

Open publisher page 0 citations

Abstract

Mixed conducting membrane SrFe0.7Cu0.3O3-δ were synthesized by sol-gel method . The crystal structures of the material and the properties of sol-gel synthesized in different conditions were studied by TG-DSC and XRD. It is found that the steady, pure cubic perovskite-structure membrane material with well-defined crystal structure can be obtained on condition that pH value of the sol is about 4, dehydrating temperature of gel is at 80 ℃, the proportion of C/Mn+ is 2, and the gel is roasted at 900 ℃ for 5 h.

About this research paper

What this paper is about

Mixed conducting membrane SrFe0.7Cu0.3O3-δ were synthesized by sol-gel method . The crystal structures of the material and the properties of sol-gel synthesized in different conditions were studied by TG-DSC and XRD. It is found that the steady, pure cubic perovskite-structure membrane material with well-defined crystal structure can be obtained on condition that pH value of the sol is about 4, dehydrating temperature of gel is at 80 ℃, the proportion of C/Mn+ is 2, and the gel is roasted at 900 ℃ for 5 h.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Mixed conducting membrane SrFe0.7Cu0.3O3-δ were synthesized by sol-gel method . The crystal structures of the material and the properties of sol-gel synthesized in different conditions were studied by TG-DSC and XRD. It is found that the steady, pure cubic perovskite-structure membrane material with well-defined crystal structure can be obtained on condition that pH value of the sol is about 4, dehydrating temperature of gel is at 80 ℃, the proportion of C/Mn+ is 2, and the gel is roasted at 900 ℃ for 5 h.

Key concepts: Sol-gel, Materials science, Membrane, Crystal (programming language), Chemical engineering, Crystal structure, Perovskite (structure), Crystallography

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation of Mixed Conducting Membrane SrFe_(0.7)Cu_(0.3)O_(3-δ) by Sol-Gel Method — Research Paper | ScholarLens