Low Temperature Flotation Experiment Study of a Certain Fine-Grained Refractory Quartz-Type Fluorite Ore
Zhang Xiao-fen
Abstract
Zhang Xiao-fen
Abstract
In view of these problems of the fine disseminated grain size of fluorite and quartz in fluorite ore in a certain place,the low recovery of fluorite and the poor quality of concentrate under the low temperature(15℃), the experiment adopted the process of one roughing one scavenging seven cleanings and concentrate of the first cleaning regrinding and re-flotation,and used self-developed ZYM as the collector of fluorite low temperature flotation. Under the pulp temperature of 5 ~10℃,the beneficiation indicators in the laboratory were as follows:fluorite ore with Ca F232.52%,fluorite concentrate with Ca F297.55%, Si O21.36%, the recovery of fluorite was 76.67%; under the pulp temperature of 10℃, the industrial indicators were as follows:fluorite ore with Ca F230.14%,fluorite concentrate with Ca F296.37%,Si O21.81%,the recovery of fluorite was 71.67%.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
In view of these problems of the fine disseminated grain size of fluorite and quartz in fluorite ore in a certain place,the low recovery of fluorite and the poor quality of concentrate under the low temperature(15℃), the experiment adopted the process of one roughing one scavenging seven cleanings and concentrate of the first cleaning regrinding and re-flotation,and used self-developed ZYM as the collector of fluorite low temperature flotation. Under the pulp temperature of 5 ~10℃,the beneficiation indicators in the laboratory were as follows:fluorite ore with Ca F232.52%,fluorite concentrate with Ca F297.55%, Si O21.36%, the recovery of fluorite was 76.67%; under the pulp temperature of 10℃, the industrial indicators were as follows:fluorite ore with Ca F230.14%,fluorite concentrate with Ca F296.37%,Si O21.81%,the recovery of fluorite was 71.67%.
Key concepts: Fluorite, Beneficiation, Quartz, Metallurgy, Mineralogy, Materials science, Geology