Deoxidation during vacuum induction melting of Ni-base superalloy
Niu Jian
Abstract
Niu Jian
Abstract
The deoxidation effect in vacuum induction melting of Ni base superalloy by using CaO crucible was studied. The influence of adding 0.02%C and 0.5%Al on deoxidation was also analyzed. Thermodynamics calculation of the deoxidation reaction in CaO crucible was done. The results show that most oxygen can be removed in melting period. In CaO crucible, adopting proper melting technology and carbon and aluminium addition amounts, oxygen content could be reduced to below 0.000?6%.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The deoxidation effect in vacuum induction melting of Ni base superalloy by using CaO crucible was studied. The influence of adding 0.02%C and 0.5%Al on deoxidation was also analyzed. Thermodynamics calculation of the deoxidation reaction in CaO crucible was done. The results show that most oxygen can be removed in melting period. In CaO crucible, adopting proper melting technology and carbon and aluminium addition amounts, oxygen content could be reduced to below 0.000?6%.
Key concepts: Crucible (geodemography), Vacuum induction melting, Superalloy, Materials science, Metallurgy, Aluminium, Base (topology), Oxygen