2012•Journal of Xiamen University of TechnologyRequires access

Fabrication and Properties of Ultrafine W-10Cu Powders and Composite

Zou Fei-fei

Open publisher page 0 citations

Abstract

W-10Cu(by weight) ultrafine powder with particle size of about 250 nm has been synthesized by chemical method,calcination and subsequent hydrogen reduction process with reaction of ammonium paratungstate and copper salt.Scanning electron microscopy(SEM) and elemental analysis results showed that the reduced temperature has a significant effect on powder morphology and purity when sintered at 1300℃ for 120 min in H2 atmosphere,W-10Cu composite derived from injection molding can reach a relative density of 99.37%,and the microstructure are homogeneous.Furthermore,the sintered W-10Cu composite exhibited excellent thermal conductivity of about 217W/(m· K),and the coefficient of thermal expansion is between 6.0×10-6~7.8×10-6K-1 in the temperature range of 25℃ to 600 ℃.

About this research paper

What this paper is about

W-10Cu(by weight) ultrafine powder with particle size of about 250 nm has been synthesized by chemical method,calcination and subsequent hydrogen reduction process with reaction of ammonium paratungstate and copper salt.Scanning electron microscopy(SEM) and elemental analysis results showed that the reduced temperature has a significant effect on powder morphology and purity when sintered at 1300℃ for 120 min in H2 atmosphere,W-10Cu composite derived from injection molding can reach a relative density of 99.37%,and the microstructure are homogeneous.Furthermore,the sintered W-10Cu composite exhibited excellent thermal conductivity of about 217W/(m· K),and the coefficient of thermal expansion is between 6.0×10-6~7.8×10-6K-1 in the temperature range of 25℃ to 600 ℃.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

W-10Cu(by weight) ultrafine powder with particle size of about 250 nm has been synthesized by chemical method,calcination and subsequent hydrogen reduction process with reaction of ammonium paratungstate and copper salt.Scanning electron microscopy(SEM) and elemental analysis results showed that the reduced temperature has a significant effect on powder morphology and purity when sintered at 1300℃ for 120 min in H2 atmosphere,W-10Cu composite derived from injection molding can reach a relative density of 99.37%,and the microstructure are homogeneous.Furthermore,the sintered W-10Cu composite exhibited excellent thermal conductivity of about 217W/(m· K),and the coefficient of thermal expansion is between 6.0×10-6~7.8×10-6K-1 in the temperature range of 25℃ to 600 ℃.

Key concepts: Materials science, Composite number, Calcination, Microstructure, Scanning electron microscope, Chemical engineering, Composite material, Molding (decorative)

Related papers

Back to paper searchBrowse research topicsOriginal source
Fabrication and Properties of Ultrafine W-10Cu Powders and Composite — Research Paper | ScholarLens