Preparation of Silica Aerogel Using Industrial Sodium Silicate as Silicon Source by Ambient Pressure Drying Method

Hongwei Li

Open publisher page 0 citations

Abstract

Using industrial grade sodium silicate as silicon source and water as reactant and solvent,SiO2 aerogels were prepared by two-step acid-base catalysis and dried at ambient pressure,45 ℃.The aerogel structure and properties were characterized.The effects of ammonia concentration,time of hydrolysis,pH value on the gel time and the aerogel properties were studied.Results show that the prepared SiO2 aerogel had typical aerogel structure characteristics and high thermal insulation properties,with the pore size of 8-12 nm,the specific surface area of 353-613 m2·g-1,particle diameter of 10-20 nm,the density of 0.09-0.15 g·cm-3,the thermal conductivity of 0.021 08 W·m-1·K-1.

About this research paper

What this paper is about

Using industrial grade sodium silicate as silicon source and water as reactant and solvent,SiO2 aerogels were prepared by two-step acid-base catalysis and dried at ambient pressure,45 ℃.The aerogel structure and properties were characterized.The effects of ammonia concentration,time of hydrolysis,pH value on the gel time and the aerogel properties were studied.Results show that the prepared SiO2 aerogel had typical aerogel structure characteristics and high thermal insulation properties,with the pore size of 8-12 nm,the specific surface area of 353-613 m2·g-1,particle diameter of 10-20 nm,the density of 0.09-0.15 g·cm-3,the thermal conductivity of 0.021 08 W·m-1·K-1.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Using industrial grade sodium silicate as silicon source and water as reactant and solvent,SiO2 aerogels were prepared by two-step acid-base catalysis and dried at ambient pressure,45 ℃.The aerogel structure and properties were characterized.The effects of ammonia concentration,time of hydrolysis,pH value on the gel time and the aerogel properties were studied.Results show that the prepared SiO2 aerogel had typical aerogel structure characteristics and high thermal insulation properties,with the pore size of 8-12 nm,the specific surface area of 353-613 m2·g-1,particle diameter of 10-20 nm,the density of 0.09-0.15 g·cm-3,the thermal conductivity of 0.021 08 W·m-1·K-1.

Key concepts: Aerogel, Sodium silicate, Materials science, Ambient pressure, Silicon, Chemical engineering, Thermal conductivity, Silicate

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation of Silica Aerogel Using Industrial Sodium Silicate as Silicon Source by Ambient Pressure Drying Method — Research Paper | ScholarLens