Abstract

Objective To enhance the bonding strength between the diamond and the substrate. Methods The diamond was pretreated with a method of degreasing—roughening—sensitizing activation—glue,and then surface was modified by electroless nickel plating on the diamond. The influence of different parameters on chemical plated nickel layer was studied by scanning electron microscopy and energy dispersive X-ray. Results The optimum technical parameters of nickel layer on the diamond about 10microns: Ni SO4·6H2O( main salt) 25 g / L,hypophosphite 30 g / L,lactic acid 15 g / L,sodium acetate 15 g / L,the stabilizer 20 mg / L,brightener 1 g / L,p H = 5. 5,temperature 85 ℃. Conclusion Hypophosphite content,thiourea content,p H,and temperature may affects the plating time,the diamond coating weight gain ratio and morphology of chemical nickel. The diamond was coated complete uniform with the optimal parameters.

About this research paper

What this paper is about

Objective To enhance the bonding strength between the diamond and the substrate. Methods The diamond was pretreated with a method of degreasing—roughening—sensitizing activation—glue,and then surface was modified by electroless nickel plating on the diamond. The influence of different parameters on chemical plated nickel layer was studied by scanning electron microscopy and energy dispersive X-ray. Results The optimum technical parameters of nickel layer on the diamond about 10microns: Ni SO4·6H2O( main salt) 25 g / L,hypophosphite 30 g / L,lactic acid 15 g / L,sodium acetate 15 g / L,the stabilizer 20 mg / L,brightener 1 g / L,p H = 5. 5,temperature 85 ℃. Conclusion Hypophosphite content,thiourea content,p H,and temperature may affects the plating time,the diamond coating weight gain ratio and morphology of chemical nickel. The diamond was coated complete uniform with the optimal parameters.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Objective To enhance the bonding strength between the diamond and the substrate. Methods The diamond was pretreated with a method of degreasing—roughening—sensitizing activation—glue,and then surface was modified by electroless nickel plating on the diamond. The influence of different parameters on chemical plated nickel layer was studied by scanning electron microscopy and energy dispersive X-ray. Results The optimum technical parameters of nickel layer on the diamond about 10microns: Ni SO4·6H2O( main salt) 25 g / L,hypophosphite 30 g / L,lactic acid 15 g / L,sodium acetate 15 g / L,the stabilizer 20 mg / L,brightener 1 g / L,p H = 5. 5,temperature 85 ℃. Conclusion Hypophosphite content,thiourea content,p H,and temperature may affects the plating time,the diamond coating weight gain ratio and morphology of chemical nickel. The diamond was coated complete uniform with the optimal parameters.

Key concepts: Sodium hypophosphite, Hypophosphite, Diamond, Nickel, Materials science, Electroless nickel plating, Scanning electron microscope, Plating (geology)