Low temperature pressureless sintering technology of Al_2O_3-SiC composites
HE Pingwe
Abstract
HE Pingwe
Abstract
6H-SiC and α-Al2O3 powders mixed as raw materials(mass ratio 7:3),adding MgO and CaO as sintering additives,Al2O3-SiC composites were prepared by pressureless sintering for 1h in hydrogen atmosphere after the green body being preoxidized for 1 h at 1 200 ℃.The effects of sintering temperature and MgO-CaO content on the sintering properties and phase composition were investigated.Result shows that when sintering temperature is 1 500 ℃,the compactness improves obviously with the increase of content of sintering addictives.With w(MgO-CaO) of 10 % added,the sample's apparent porosity is 0.1%.When the green body is preoxidized,CaAl2Si2O8 and Mg2Al4Si5O18 are generated by the reaction of MgO-CaO with α-Al2O3,SiO2.During the sintering process,CaAl2Si2O8 and MgAl2O4 form liquid glass phase which promotes sintering and deposits α-Al2O3.The sample's crystal phases are 6H-SiC and α-Al2O3 at 1 500 ℃.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
6H-SiC and α-Al2O3 powders mixed as raw materials(mass ratio 7:3),adding MgO and CaO as sintering additives,Al2O3-SiC composites were prepared by pressureless sintering for 1h in hydrogen atmosphere after the green body being preoxidized for 1 h at 1 200 ℃.The effects of sintering temperature and MgO-CaO content on the sintering properties and phase composition were investigated.Result shows that when sintering temperature is 1 500 ℃,the compactness improves obviously with the increase of content of sintering addictives.With w(MgO-CaO) of 10 % added,the sample's apparent porosity is 0.1%.When the green body is preoxidized,CaAl2Si2O8 and Mg2Al4Si5O18 are generated by the reaction of MgO-CaO with α-Al2O3,SiO2.During the sintering process,CaAl2Si2O8 and MgAl2O4 form liquid glass phase which promotes sintering and deposits α-Al2O3.The sample's crystal phases are 6H-SiC and α-Al2O3 at 1 500 ℃.
Key concepts: Sintering, Materials science, Pressureless sintering, Raw material, Composite material, Porosity, Phase (matter), Green body