Alumina ceramics is densely sintered at 1450℃ by using CaO-MgO-SiO2 glass(CMS-G) and TiO2 as sintering assistant.The effect that the weight content of CMS-G and TiO2 to sintering character,and fine texture and sintering kinetics of alumina ceramics is studied.The results show that CMS-G and TiO2 can accelerate density of alumina ceramics effectively,the relative density of alumina ceramics is up to 98.25%,when content of CMS-G is 3% and TiO2 is 1%.Sintering process is controlled by diffusion,and activation energy of liquid phase sintering is 113.4kJ/mol.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Alumina ceramics is densely sintered at 1450℃ by using CaO-MgO-SiO2 glass(CMS-G) and TiO2 as sintering assistant.The effect that the weight content of CMS-G and TiO2 to sintering character,and fine texture and sintering kinetics of alumina ceramics is studied.The results show that CMS-G and TiO2 can accelerate density of alumina ceramics effectively,the relative density of alumina ceramics is up to 98.25%,when content of CMS-G is 3% and TiO2 is 1%.Sintering process is controlled by diffusion,and activation energy of liquid phase sintering is 113.4kJ/mol.
Key concepts: Sintering, Materials science, Ceramic, Activation energy, Alumina ceramic, Liquid phase, Kinetics, Relative density