Research on Nitrogen-controlling Process for Melting Nitrogen-contained 316L Stainless Steel in VIM Furnace

Wang Mingb

Open publisher page 0 citations

Abstract

The influence of nitrogen partial pressure on the nitrogen solubility in nitrogen-contained 316Lstainless steel was studied.Results showed that the nitrogen solubility increased with increasing the nitrogen partial pressure.The controlling nitrogen process was investigated by adding FeCrN(Cr:60%,N:6%)with(0.2-0.8)×105 Pa nitrogen atmosphere in 500kg vacuum induction furnace for melting nitrogen-contained 316Lstainless steel(N:0.1%-0.2%).Results showed that with the nitrogen pressure(0.2-0.3)×105 Pa the yield of nitrogen was 65%-80%.And when the nitrogen pressure was to(0.5-0.6)×105 Pa,the yield of nitrogen was 80%-90%.With increasing nitrogen pressure to 0.8×105 Pa the yield of nitrogen was up to 100%.

About this research paper

What this paper is about

The influence of nitrogen partial pressure on the nitrogen solubility in nitrogen-contained 316Lstainless steel was studied.Results showed that the nitrogen solubility increased with increasing the nitrogen partial pressure.The controlling nitrogen process was investigated by adding FeCrN(Cr:60%,N:6%)with(0.2-0.8)×105 Pa nitrogen atmosphere in 500kg vacuum induction furnace for melting nitrogen-contained 316Lstainless steel(N:0.1%-0.2%).Results showed that with the nitrogen pressure(0.2-0.3)×105 Pa the yield of nitrogen was 65%-80%.And when the nitrogen pressure was to(0.5-0.6)×105 Pa,the yield of nitrogen was 80%-90%.With increasing nitrogen pressure to 0.8×105 Pa the yield of nitrogen was up to 100%.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The influence of nitrogen partial pressure on the nitrogen solubility in nitrogen-contained 316Lstainless steel was studied.Results showed that the nitrogen solubility increased with increasing the nitrogen partial pressure.The controlling nitrogen process was investigated by adding FeCrN(Cr:60%,N:6%)with(0.2-0.8)×105 Pa nitrogen atmosphere in 500kg vacuum induction furnace for melting nitrogen-contained 316Lstainless steel(N:0.1%-0.2%).Results showed that with the nitrogen pressure(0.2-0.3)×105 Pa the yield of nitrogen was 65%-80%.And when the nitrogen pressure was to(0.5-0.6)×105 Pa,the yield of nitrogen was 80%-90%.With increasing nitrogen pressure to 0.8×105 Pa the yield of nitrogen was up to 100%.

Key concepts: Nitrogen, Solubility, Materials science, Yield (engineering), Partial pressure, Vacuum induction melting, Nitrogen gas, Metallurgy

Related papers

Back to paper searchBrowse research topicsOriginal source
Research on Nitrogen-controlling Process for Melting Nitrogen-contained 316L Stainless Steel in VIM Furnace — Research Paper | ScholarLens