Active flux for austenitic stainless steel tungsten inert-gas welding

Wang Yong-shan

Open publisher page 0 citations

Abstract

Active flux for austenitic stainless steel TIG(tungsten inert-gas) welding was studied using the orthogonal method. With the resulting flux and heat input of 1.01 kJ/mm ,the austenitic stainless steel of 5 mm thickness was penetrated by TIG welding without beveling.When increasing heat input to 1.95 kJ/mm, the steel of 8mm thickness was penetrated. The arc was steady during welding,and appearance of weld is good. The flux has a function of suppressing alloy elements to escape from weld pool, so that the weight percentages of Cr and Ni in the A-TIG(active-tungsten inert-gas welding) weld metal are descended very slightly. The microstructure of the A-TIG welds is almost the same as that of the TIG welds. The hardness of the former is somewhate higher than that of the later.

About this research paper

What this paper is about

Active flux for austenitic stainless steel TIG(tungsten inert-gas) welding was studied using the orthogonal method. With the resulting flux and heat input of 1.01 kJ/mm ,the austenitic stainless steel of 5 mm thickness was penetrated by TIG welding without beveling.When increasing heat input to 1.95 kJ/mm, the steel of 8mm thickness was penetrated. The arc was steady during welding,and appearance of weld is good. The flux has a function of suppressing alloy elements to escape from weld pool, so that the weight percentages of Cr and Ni in the A-TIG(active-tungsten inert-gas welding) weld metal are descended very slightly. The microstructure of the A-TIG welds is almost the same as that of the TIG welds. The hardness of the former is somewhate higher than that of the later.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Active flux for austenitic stainless steel TIG(tungsten inert-gas) welding was studied using the orthogonal method. With the resulting flux and heat input of 1.01 kJ/mm ,the austenitic stainless steel of 5 mm thickness was penetrated by TIG welding without beveling.When increasing heat input to 1.95 kJ/mm, the steel of 8mm thickness was penetrated. The arc was steady during welding,and appearance of weld is good. The flux has a function of suppressing alloy elements to escape from weld pool, so that the weight percentages of Cr and Ni in the A-TIG(active-tungsten inert-gas welding) weld metal are descended very slightly. The microstructure of the A-TIG welds is almost the same as that of the TIG welds. The hardness of the former is somewhate higher than that of the later.

Key concepts: Gas tungsten arc welding, Welding, Materials science, Metallurgy, Inert gas, Tungsten, Austenite, Arc welding

Related papers

Back to paper searchBrowse research topicsOriginal source
Active flux for austenitic stainless steel tungsten inert-gas welding — Research Paper | ScholarLens