2006Rengong jingti xuebaoRequires access

Influence of Sintering Technique on Mechanical Properties and Microstructure of B_4C/TiB_2/Mo/C Composite

Changxia Liu

Open publisher page 1 citations

Abstract

80.6wt.%B_4C/11.6wt.%TiB_2/4.7wt%Mo/3wt.%C ceramic composite is fabricated by hot-pressing sintering and the effect of sintering temperature,holding time and pressure on mechanical properties and microstructure of the composite are analyzed.The temperature is raised from 1800℃ to 1950℃,the holding time ranges from 15min to 60min and the pressure is 30-35MPa.The strength,hardness,toughness and densification of the composite prepared by the optimized process of 1900℃ under 35MPa for 45min are 705MPa,20.6GPa,3.82MPa·m~1/2,98.2%,respectively.

About this research paper

What this paper is about

80.6wt.%B_4C/11.6wt.%TiB_2/4.7wt%Mo/3wt.%C ceramic composite is fabricated by hot-pressing sintering and the effect of sintering temperature,holding time and pressure on mechanical properties and microstructure of the composite are analyzed.The temperature is raised from 1800℃ to 1950℃,the holding time ranges from 15min to 60min and the pressure is 30-35MPa.The strength,hardness,toughness and densification of the composite prepared by the optimized process of 1900℃ under 35MPa for 45min are 705MPa,20.6GPa,3.82MPa·m~1/2,98.2%,respectively.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

80.6wt.%B_4C/11.6wt.%TiB_2/4.7wt%Mo/3wt.%C ceramic composite is fabricated by hot-pressing sintering and the effect of sintering temperature,holding time and pressure on mechanical properties and microstructure of the composite are analyzed.The temperature is raised from 1800℃ to 1950℃,the holding time ranges from 15min to 60min and the pressure is 30-35MPa.The strength,hardness,toughness and densification of the composite prepared by the optimized process of 1900℃ under 35MPa for 45min are 705MPa,20.6GPa,3.82MPa·m~1/2,98.2%,respectively.

Key concepts: Materials science, Microstructure, Sintering, Composite number, Composite material, Ceramic, Fracture toughness, Toughness