With Y2O3:Al2O3(A 2:3; B 3:1 total amount 15wt%) as sintering additives and SiC as the second phase,high flexural strength Si3N4/SiC composite ceramics were prepared via nitridation of Si powder. The phase composition,relative density,microstructure as well as mechanical properties were investigated. The experimental results showed that the α→β-Si3N4 phase transformation could be completed at 1700℃ for 2 h with sintering additives A or B. With the sintering additive A and 5wt% SiC addition,the maximum relative density of 94.8% and maximum flexural strength of 521.8 MPa were obtained for the Si3N4/SiC composite ceramics. As compared with the specimen without SiC addition which flexural strength was 338.7 MPa,flexural strength of the above mentioned Si3N4/SiC composite ceramics was improved by 54.1%. SiC powder can effectively improve the mechanical properties of the specimen and the fracture of Si3N4/SiC composite ceramics followed the typical intergranular fractural mode.

About this research paper

What this paper is about

With Y2O3:Al2O3(A 2:3; B 3:1 total amount 15wt%) as sintering additives and SiC as the second phase,high flexural strength Si3N4/SiC composite ceramics were prepared via nitridation of Si powder. The phase composition,relative density,microstructure as well as mechanical properties were investigated. The experimental results showed that the α→β-Si3N4 phase transformation could be completed at 1700℃ for 2 h with sintering additives A or B. With the sintering additive A and 5wt% SiC addition,the maximum relative density of 94.8% and maximum flexural strength of 521.8 MPa were obtained for the Si3N4/SiC composite ceramics. As compared with the specimen without SiC addition which flexural strength was 338.7 MPa,flexural strength of the above mentioned Si3N4/SiC composite ceramics was improved by 54.1%. SiC powder can effectively improve the mechanical properties of the specimen and the fracture of Si3N4/SiC composite ceramics followed the typical intergranular fractural mode.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

With Y2O3:Al2O3(A 2:3; B 3:1 total amount 15wt%) as sintering additives and SiC as the second phase,high flexural strength Si3N4/SiC composite ceramics were prepared via nitridation of Si powder. The phase composition,relative density,microstructure as well as mechanical properties were investigated. The experimental results showed that the α→β-Si3N4 phase transformation could be completed at 1700℃ for 2 h with sintering additives A or B. With the sintering additive A and 5wt% SiC addition,the maximum relative density of 94.8% and maximum flexural strength of 521.8 MPa were obtained for the Si3N4/SiC composite ceramics. As compared with the specimen without SiC addition which flexural strength was 338.7 MPa,flexural strength of the above mentioned Si3N4/SiC composite ceramics was improved by 54.1%. SiC powder can effectively improve the mechanical properties of the specimen and the fracture of Si3N4/SiC composite ceramics followed the typical intergranular fractural mode.

Key concepts: Materials science, Flexural strength, Sintering, Composite number, Ceramic, Composite material, Relative density, Microstructure

Related papers

Back to paper searchBrowse research topicsOriginal source
Mechanical Properties of Reaction-bonded Si_3N_4/SiC Composite Ceramics — Research Paper | ScholarLens