Preparation of Horniness Oxidized Wax by Catalytic Oxidation

Hongbo Yu

Open publisher page 0 citations

Abstract

The catalytic oxidation experiments were carried out to prepare the horniness oxidized wax from paraffin wax and polyethylene. The results show that good products can be obtained under the following conditions: reaction temperature 170 ℃,reaction time 7 h,mass ratio of paraffin wax and polyethylene 7∶3,the amount of catalyst 0.01%,the amount of additive 1.0%,the air flow 0.20 m3/h.acid number of the product was 9.82 mg(KOH)/g,saponification number is 79.19 mg(KOH)/g,penetration is 9.2(0.1 mm),melting point was 87.4 ℃,index of refraction(75 ℃) was 1.453 6.As compared with natural hard wax(carnauba wax),their properties were quite similar each other.

About this research paper

What this paper is about

The catalytic oxidation experiments were carried out to prepare the horniness oxidized wax from paraffin wax and polyethylene. The results show that good products can be obtained under the following conditions: reaction temperature 170 ℃,reaction time 7 h,mass ratio of paraffin wax and polyethylene 7∶3,the amount of catalyst 0.01%,the amount of additive 1.0%,the air flow 0.20 m3/h.acid number of the product was 9.82 mg(KOH)/g,saponification number is 79.19 mg(KOH)/g,penetration is 9.2(0.1 mm),melting point was 87.4 ℃,index of refraction(75 ℃) was 1.453 6.As compared with natural hard wax(carnauba wax),their properties were quite similar each other.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The catalytic oxidation experiments were carried out to prepare the horniness oxidized wax from paraffin wax and polyethylene. The results show that good products can be obtained under the following conditions: reaction temperature 170 ℃,reaction time 7 h,mass ratio of paraffin wax and polyethylene 7∶3,the amount of catalyst 0.01%,the amount of additive 1.0%,the air flow 0.20 m3/h.acid number of the product was 9.82 mg(KOH)/g,saponification number is 79.19 mg(KOH)/g,penetration is 9.2(0.1 mm),melting point was 87.4 ℃,index of refraction(75 ℃) was 1.453 6.As compared with natural hard wax(carnauba wax),their properties were quite similar each other.

Key concepts: Wax, Carnauba wax, Catalysis, Saponification, Polyethylene, Melting point, Penetration (warfare), Paraffin wax

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation of Horniness Oxidized Wax by Catalytic Oxidation — Research Paper | ScholarLens