An experimental study on the transition between fretting and reciprocating sliding wear has been carried out using a AISI 52100 steel ball of 60mm diameter rubbed against a flat specimen made from the same steel under 300 N normal load. Wear coefficient, coefficient of friction and wear mark morphology were analyzed and debris observation was made.The results show that in addition to wear coefficient friction coefficient and wear mark morphology also have to some extent changes before and after the transition. A transition probably occurs between 70 μm and 100 μm under the present conditions.

About this research paper

What this paper is about

An experimental study on the transition between fretting and reciprocating sliding wear has been carried out using a AISI 52100 steel ball of 60mm diameter rubbed against a flat specimen made from the same steel under 300 N normal load. Wear coefficient, coefficient of friction and wear mark morphology were analyzed and debris observation was made.The results show that in addition to wear coefficient friction coefficient and wear mark morphology also have to some extent changes before and after the transition. A transition probably occurs between 70 μm and 100 μm under the present conditions.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

An experimental study on the transition between fretting and reciprocating sliding wear has been carried out using a AISI 52100 steel ball of 60mm diameter rubbed against a flat specimen made from the same steel under 300 N normal load. Wear coefficient, coefficient of friction and wear mark morphology were analyzed and debris observation was made.The results show that in addition to wear coefficient friction coefficient and wear mark morphology also have to some extent changes before and after the transition. A transition probably occurs between 70 μm and 100 μm under the present conditions.

Key concepts: Reciprocating motion, Fretting, Materials science, Friction coefficient, Coefficient of friction, Metallurgy, Fretting wear, Frictional coefficient

Related papers

Back to paper searchBrowse research topicsOriginal source
Study on GCr15 Friction Behavior before and after the Transition from Fretting to Reciprocating Sliding Wear — Research Paper | ScholarLens