Effects of sintering temperature on piezoelectric property of 0.55Pb(Ni_(1/3)Nb_(2/3))O_3-0.45Pb(Zr_(0.3)Ti_(0.7))O_3 ceramics
Ji Hongli
Abstract
Ji Hongli
Abstract
0.55Pb(Ni1/3Nb2/3)O3-0.45Pb(Zr0.3Ti0.7)O3 (0.55PNN-0.45PZT) piezoelectric ceramics are high-performance piezoelectric materials,which are widely used to fabricate the fibers with Pt core and other electronic devices.In order to improve the electrical properties of the piezoelectric ceramic fibers,the 0.55PNN-0.45PZT ceramics with high electrical properties were fabricated by the traditional sintering method in this study.The effects of sintering temperature on the phase structure,microstructure and electrical properties of material have been investigated.High electrical properties ceramic were fabricated by optimizing the sintering temperature.The highest piezoelectric properties were achieved when the ceramics were sintered at 1200℃,and their values were ρ=8.12g/cm3,d33=850pC/N,kp=0.62,er=7317,tanδ=0.033,and Qm=41.66.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
0.55Pb(Ni1/3Nb2/3)O3-0.45Pb(Zr0.3Ti0.7)O3 (0.55PNN-0.45PZT) piezoelectric ceramics are high-performance piezoelectric materials,which are widely used to fabricate the fibers with Pt core and other electronic devices.In order to improve the electrical properties of the piezoelectric ceramic fibers,the 0.55PNN-0.45PZT ceramics with high electrical properties were fabricated by the traditional sintering method in this study.The effects of sintering temperature on the phase structure,microstructure and electrical properties of material have been investigated.High electrical properties ceramic were fabricated by optimizing the sintering temperature.The highest piezoelectric properties were achieved when the ceramics were sintered at 1200℃,and their values were ρ=8.12g/cm3,d33=850pC/N,kp=0.62,er=7317,tanδ=0.033,and Qm=41.66.
Key concepts: Materials science, Sintering, Piezoelectricity, Ceramic, Microstructure, Composite material, Phase (matter), Organic chemistry