Bleaching process to wool/flax blended yarn with peracetic acid

Ren Hui-ming

Open publisher page 1 citations

Abstract

Bleaching process to wool/flax blended yarn with environmental friendly peracetic acid was carried out.On the basis of studying the bleaching performance influenced by factors such as peracetic acid concentration,bleaching temperature,pH value,treatment time and stabilizer consumption,the optimal bleaching technology was determined.That were peracetic acid 8 g/L,sodium pyrophosphate 1.5 g/L,pH value 6.5,bleaching at 75 ℃ for 80 minutes.Results of performance test indicated that the beaching condition to wool/flax blended yarn with peracetic acid was mild,and having little damage to the blended yarn,being conducive to environmental protection and following knitting,weaving,dyeing and finishing.The feasibility of technology was turned out.

About this research paper

What this paper is about

Bleaching process to wool/flax blended yarn with environmental friendly peracetic acid was carried out.On the basis of studying the bleaching performance influenced by factors such as peracetic acid concentration,bleaching temperature,pH value,treatment time and stabilizer consumption,the optimal bleaching technology was determined.That were peracetic acid 8 g/L,sodium pyrophosphate 1.5 g/L,pH value 6.5,bleaching at 75 ℃ for 80 minutes.Results of performance test indicated that the beaching condition to wool/flax blended yarn with peracetic acid was mild,and having little damage to the blended yarn,being conducive to environmental protection and following knitting,weaving,dyeing and finishing.The feasibility of technology was turned out.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Bleaching process to wool/flax blended yarn with environmental friendly peracetic acid was carried out.On the basis of studying the bleaching performance influenced by factors such as peracetic acid concentration,bleaching temperature,pH value,treatment time and stabilizer consumption,the optimal bleaching technology was determined.That were peracetic acid 8 g/L,sodium pyrophosphate 1.5 g/L,pH value 6.5,bleaching at 75 ℃ for 80 minutes.Results of performance test indicated that the beaching condition to wool/flax blended yarn with peracetic acid was mild,and having little damage to the blended yarn,being conducive to environmental protection and following knitting,weaving,dyeing and finishing.The feasibility of technology was turned out.

Key concepts: Peracetic acid, Wool, Dyeing, Yarn, Pulp and paper industry, Materials science, Textile, Weaving

Related papers

Back to paper searchBrowse research topicsOriginal source
Bleaching process to wool/flax blended yarn with peracetic acid — Research Paper | ScholarLens