Study on Friction and Wear Characteristics of Cu-0.8Cr-0.14Zr-0.06Mg Alloy
Jie Wang
Abstract
Jie Wang
Abstract
The electrical sliding wear of the Cu-0.8Cr-0.14Zr-0.06Mg alloy are studied by loading different lining speed and electric current in this article.The alloy sliding worn surfaces and wear mechanism are observed and analyzed by optical microscopy and SEM.The results show that the alloy solved at 920 ℃ for 30 min and aging at 450 ℃ for 180 min behaves a linear relationship between the wear volume and running speed,and the wear mechanism is adhesive wear and abrasive wear.The wear mechanism becomes adhesive wear,abrasive wear and arc induced wear after loading current.And as the current increases,the adhesive wear and arc induced wear is becoming increasingly serious.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The electrical sliding wear of the Cu-0.8Cr-0.14Zr-0.06Mg alloy are studied by loading different lining speed and electric current in this article.The alloy sliding worn surfaces and wear mechanism are observed and analyzed by optical microscopy and SEM.The results show that the alloy solved at 920 ℃ for 30 min and aging at 450 ℃ for 180 min behaves a linear relationship between the wear volume and running speed,and the wear mechanism is adhesive wear and abrasive wear.The wear mechanism becomes adhesive wear,abrasive wear and arc induced wear after loading current.And as the current increases,the adhesive wear and arc induced wear is becoming increasingly serious.
Key concepts: Adhesive wear, Abrasive, Materials science, Alloy, Adhesive, Metallurgy, Arc (geometry), Mechanism (biology)