SEPARATION OF Cu, Ni AND Co FROM AMMONIA SOLUTION BY SOLVENT EXTRACTION

Chengyan Wang

Open publisher page 0 citations

Abstract

Copper, nickel and cobalt are separated from ammonia solution by PT5050 solvent extraction The extraction rates of Cu 2+ and Ni 2+ reach to 99 5%, and Co 3+ is in the raffinate The stripping rate of Ni 2+ reaches to 99% by selectivity stripping, and Cu 2+ content in the Ni 2+ stripping liquor is 0 001g/L, It applys to produce cathode nickel Copper is stripped by high concentration solution (180 g/L H 2SO 4), and producing cathode copper or copper sulfate Cobalt in raffinate is cemented by Na 2S, the grade of cobalt in precipitate is higher than 40%, and the recovery is higher than 96%

About this research paper

What this paper is about

Copper, nickel and cobalt are separated from ammonia solution by PT5050 solvent extraction The extraction rates of Cu 2+ and Ni 2+ reach to 99 5%, and Co 3+ is in the raffinate The stripping rate of Ni 2+ reaches to 99% by selectivity stripping, and Cu 2+ content in the Ni 2+ stripping liquor is 0 001g/L, It applys to produce cathode nickel Copper is stripped by high concentration solution (180 g/L H 2SO 4), and producing cathode copper or copper sulfate Cobalt in raffinate is cemented by Na 2S, the grade of cobalt in precipitate is higher than 40%, and the recovery is higher than 96%

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Copper, nickel and cobalt are separated from ammonia solution by PT5050 solvent extraction The extraction rates of Cu 2+ and Ni 2+ reach to 99 5%, and Co 3+ is in the raffinate The stripping rate of Ni 2+ reaches to 99% by selectivity stripping, and Cu 2+ content in the Ni 2+ stripping liquor is 0 001g/L, It applys to produce cathode nickel Copper is stripped by high concentration solution (180 g/L H 2SO 4), and producing cathode copper or copper sulfate Cobalt in raffinate is cemented by Na 2S, the grade of cobalt in precipitate is higher than 40%, and the recovery is higher than 96%

Key concepts: Raffinate, Cobalt, Copper, Stripping (fiber), Nickel, Ammonia, Extraction (chemistry), Chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
SEPARATION OF Cu, Ni AND Co FROM AMMONIA SOLUTION BY SOLVENT EXTRACTION — Research Paper | ScholarLens