Study on High Quality Sapphire Crystals by Kyropulos Method
Baodong Chen
Abstract
Baodong Chen
Abstract
A high quality sapphire crystal oriented along was grown by Kyropulos method.The dislocations density of the sapphire crystal is about 2×103-1.3×104 /cm2.And with the help of LA-ICP-MS,a precise measurement about sapphire crystal impurities was carried out and the data was analyzed.The transmission spectra tested from 600 nm to 1200 nm the transmission of sapphire crystal is above 80 percent,while from 1200 nm to 3000 nm it is above 85 percent.The high quality sapphire crystals grown by Kyropulos method have been utilized in some commercial products and show good performance.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
A high quality sapphire crystal oriented along was grown by Kyropulos method.The dislocations density of the sapphire crystal is about 2×103-1.3×104 /cm2.And with the help of LA-ICP-MS,a precise measurement about sapphire crystal impurities was carried out and the data was analyzed.The transmission spectra tested from 600 nm to 1200 nm the transmission of sapphire crystal is above 80 percent,while from 1200 nm to 3000 nm it is above 85 percent.The high quality sapphire crystals grown by Kyropulos method have been utilized in some commercial products and show good performance.
Key concepts: Sapphire, Materials science, Crystal (programming language), Impurity, Czochralski method, Quality (philosophy), Optoelectronics, Optics