Study on the experiment of thermal insulation glazed hollow bead concrete mixing with haydite
Di Wu
Abstract
Di Wu
Abstract
Based on the experiment of thermal insulation glazed hollow bead concrete,the paper exerts the way of orthogonal experiment,and the law effect of mixing amount of glazed hollow bead,density of glazed hollow bead,amount of haydite,strength of cement,amount of cement,amount of sand,and admixture on thermal conductivity and compressive strength of concrete has been analyzed.The result shows that it is feasible to compose glazed hollow bead and haydite concrete by mixing haydite into thermal insulation glazed hollow bead concrete.Its max.compressive strength is 45.58 MPa and the min thermal conductivity is 0.159 W/(m·K).
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Based on the experiment of thermal insulation glazed hollow bead concrete,the paper exerts the way of orthogonal experiment,and the law effect of mixing amount of glazed hollow bead,density of glazed hollow bead,amount of haydite,strength of cement,amount of cement,amount of sand,and admixture on thermal conductivity and compressive strength of concrete has been analyzed.The result shows that it is feasible to compose glazed hollow bead and haydite concrete by mixing haydite into thermal insulation glazed hollow bead concrete.Its max.compressive strength is 45.58 MPa and the min thermal conductivity is 0.159 W/(m·K).
Key concepts: Bead, Materials science, Mixing (physics), Composite material, Thermal conductivity, Compressive strength, Thermal insulation, Cement