Eliminate Lack of Surface Hardness of Carburizing Parts by Preoxidation at 450

He Xiu

Open publisher page 0 citations

Abstract

By preoxidizing at 450℃ for an hour before carburizing quenching, elimination of uneven depth of carburizing zone and lack of surface hardness that varied in a great range since the sealed multipurpose chamber furnace was imported,the quality of parts treated with the furnace is stable and good benefit was obtained.

About this research paper

What this paper is about

By preoxidizing at 450℃ for an hour before carburizing quenching, elimination of uneven depth of carburizing zone and lack of surface hardness that varied in a great range since the sealed multipurpose chamber furnace was imported,the quality of parts treated with the furnace is stable and good benefit was obtained.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

By preoxidizing at 450℃ for an hour before carburizing quenching, elimination of uneven depth of carburizing zone and lack of surface hardness that varied in a great range since the sealed multipurpose chamber furnace was imported,the quality of parts treated with the furnace is stable and good benefit was obtained.

Key concepts: Carburizing, Hardness, Quenching (fluorescence), Metallurgy, Materials science, Case hardening, Fluorescence, Physics