1992Acta Metallurgica SinicaRequires access

RECALESCENCE AND SOLIDIFICATION MICROSTRUCTURE OF HIGHLY UNDERCOOLED ALLOY Ni_(68)B_(21)Si_(11).

Zhou Yaohe

Open publisher page 0 citations

Abstract

One, two and three recalescence events in the solidification of highly undercooled Ni_(68)B_(21)Si_(11) alloy melt and the conditions of undercooled together with the effect on solidification morphologies were revealed. The solidification morphologies of the undercooled alloy may be examined in the light of two aspects, i.e., growth of either Ni_3B Ni_6Si_2B and Ni_2B eutectic or dendrite cluster with Ni_3B as leading phase. When the degree of undercooling below 200 or over 310 K, the solidification of alloy is accompannied by one recalescene only, and the crystals grow according to the first mode of solidification. While undercooling at other temperatures, two or three events of recalescence may occur and the dendrite cluster may solidify.

About this research paper

What this paper is about

One, two and three recalescence events in the solidification of highly undercooled Ni_(68)B_(21)Si_(11) alloy melt and the conditions of undercooled together with the effect on solidification morphologies were revealed. The solidification morphologies of the undercooled alloy may be examined in the light of two aspects, i.e., growth of either Ni_3B Ni_6Si_2B and Ni_2B eutectic or dendrite cluster with Ni_3B as leading phase. When the degree of undercooling below 200 or over 310 K, the solidification of alloy is accompannied by one recalescene only, and the crystals grow according to the first mode of solidification. While undercooling at other temperatures, two or three events of recalescence may occur and the dendrite cluster may solidify.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

One, two and three recalescence events in the solidification of highly undercooled Ni_(68)B_(21)Si_(11) alloy melt and the conditions of undercooled together with the effect on solidification morphologies were revealed. The solidification morphologies of the undercooled alloy may be examined in the light of two aspects, i.e., growth of either Ni_3B Ni_6Si_2B and Ni_2B eutectic or dendrite cluster with Ni_3B as leading phase. When the degree of undercooling below 200 or over 310 K, the solidification of alloy is accompannied by one recalescene only, and the crystals grow according to the first mode of solidification. While undercooling at other temperatures, two or three events of recalescence may occur and the dendrite cluster may solidify.

Key concepts: Recalescence, Supercooling, Materials science, Eutectic system, Alloy, Dendrite (mathematics), Microstructure, Metallurgy

Related papers

Back to paper searchBrowse research topicsOriginal source
RECALESCENCE AND SOLIDIFICATION MICROSTRUCTURE OF HIGHLY UNDERCOOLED ALLOY Ni_(68)B_(21)Si_(11). — Research Paper | ScholarLens