Flotation of low grade scheelite

Deng Shuangli

Open publisher page 0 citations

Abstract

While the content of WO3 in scheelite was about 0.06%,the process flow of rough flotation at the room temperature-thickening of coarse concentrate-reagent removing from concentrated slurry at high temperature-cleaning flotation at room temperature was applied,and then tungsten concentrate with the grade of 25% and the recovery rate of 70% was obtained.

About this research paper

What this paper is about

While the content of WO3 in scheelite was about 0.06%,the process flow of rough flotation at the room temperature-thickening of coarse concentrate-reagent removing from concentrated slurry at high temperature-cleaning flotation at room temperature was applied,and then tungsten concentrate with the grade of 25% and the recovery rate of 70% was obtained.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

While the content of WO3 in scheelite was about 0.06%,the process flow of rough flotation at the room temperature-thickening of coarse concentrate-reagent removing from concentrated slurry at high temperature-cleaning flotation at room temperature was applied,and then tungsten concentrate with the grade of 25% and the recovery rate of 70% was obtained.

Key concepts: Scheelite, Reagent, Slurry, Tungsten, Thickening, Metallurgy, Materials science, Mineralogy

Related papers

Back to paper searchBrowse research topicsOriginal source
Flotation of low grade scheelite — Research Paper | ScholarLens